MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Braskem EP 548S Injection Molding Polypropylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Description: EP 548S is a heterophasic copolymer of high fluidity, which provides high rigidity and resistance to the average impact. Due to its good organoleptic properties, it is recommended for use in packaging of food products that require low transfer of odor and taste.

Applications: Injection Molding of toys, thin-walled rigid containers, home utilities and others.

Information provided by Braskem

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.903 g/cc0.0326 lb/in³ASTM D792
Melt Flow 44 g/10 min
@Load 2.16 kg,
Temperature 230 °C
44 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7171ASTM D2240
Tensile Strength, Yield 28.0 MPa4060 psiASTM D638
Elongation at Yield 7.0 %7.0 %ASTM D638
Flexural Modulus, 1% Secant 1350 MPa196000 psiASTM D790
Izod Impact, Notched  0.350 J/cm
@Temperature -20.0 °C
0.656 ft-lb/in
@Temperature -4.00 °F
ASTM D256
 0.550 J/cm
@Temperature 23.0 °C
1.03 ft-lb/in
@Temperature 73.4 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 105 °C221 °FASTM D648
Vicat Softening Point 145 °C
@Load 1.02 kg
293 °F
@Load 2.25 lb
ASTM D1525

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Flint Hills P6G2N-095 Impact Copolymer Polypropylene
Ineos L12Z-01 Polypropylene Impact Copolymer
Ineos N00M-00 Polypropylene Impact Copolymer
Ineos N05U-00 Polypropylene Impact Copolymer
LyondellBasell Alathon® M5352 High Density Polyethylene, Injection Molding Grade

PBRASK2130 / 200011

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.