MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ineos L12Z-01 Polypropylene Impact Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Grade L12Z-01 is a nucleated and antistatic polypropylene copolymer with a medium melt flow rate that provides an excellent balance of stiffness and impact. It is especially formulated to help provide superior gloss for end-use applications. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.

Applications

  • Consumer products
  • Housewares
  • Toys
Benefits
  • Medium impact resistance
  • Excellent balance of stiffness and impact
  • Superior gloss
  • Fast cycling

Key Words: Excellent balance of stiffness and impact
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.905 g/cc0.0327 lb/in³ASTM D792
Melt Flow 12 g/10 min
@Load 2.16 kg,
Temperature 230 °C
12 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 8484ASTM D785
Tensile Strength at Break 17.2 MPa2490 psi2.0 in/min; ASTM D638
Tensile Strength, Yield 26.5 MPa3850 psi2.0 in/min; ASTM D638
Elongation at Break 160 %160 %2.0 in/min; ASTM D638
Elongation at Yield 7.0 %7.0 %2.0 in/min; ASTM D638
Flexural Modulus, 1% Secant 1300 MPa188000 psiASTM D790A
Izod Impact, Notched  0.481 J/cm
@Temperature -20.0 °C
0.900 ft-lb/in
@Temperature -4.00 °F
ASTM D256
 1.82 J/cm
@Temperature 22.8 °C
3.40 ft-lb/in
@Temperature 73.0 °F
ASTM D256
Izod Impact, Notched (ISO)  5.00 kJ/m²
@Temperature -20.0 °C
2.38 ft-lb/in²
@Temperature -4.00 °F
Area; ASTM D256
 18.0 kJ/m²
@Temperature 22.8 °C
8.57 ft-lb/in²
@Temperature 73.0 °F
Area; ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 104 °C220 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 53.9 °C129 °FUnannealed; ASTM D648
Vicat Softening Point 149 °C300 °FASTM D1525
UL RTI, Electrical 65.0 °C
@Thickness 1.52 mm
149 °F
@Thickness 0.0600 in
UL 746
UL RTI, Mechanical with Impact 65.0 °C
@Thickness 1.52 mm
149 °F
@Thickness 0.0600 in
UL 746
UL RTI, Mechanical without Impact 65.0 °C
@Thickness 1.52 mm
149 °F
@Thickness 0.0600 in
UL 746
Flammability, UL94 HB
@Thickness 1.52 mm
HB
@Thickness 0.0600 in
 
Optical PropertiesMetricEnglishComments
Gloss 81 %81 %60°; ASTM D2457
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
 
Descriptive Properties
processInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Pinnacle Polymers 3220 Impact Polypropylene Copolymer, Injection Molding Grade
Pinnacle Polymers 3208 High Impact Polypropylene Copolymer, Injection Molding Grade
Pinnacle Polymers 2135 Impact Polypropylene Copolymer, Injection Molding Grade
Pinnacle Polymers 2135 H Medium Impact Polypropylene Copolymer, Injection Molding Grade
Pinnacle Polymers 2150 H Medium Impact Polypropylene Copolymer, Injection Molding Grade

PINEOS002 / 48170

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.