System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
ExxonMobil Escorene® UL-7505 EVA Copolymer, Adhesive and Sealant Grade
(discontinued **)
Categories:
Polymer
;
Thermoplastic
;
Ethylene Vinyl Acetate
;
Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade
Material Notes:
Data provided by the manufacturer, Exxon Chemical.
A 19.2% vinyl acetate copolymer
Applications:
Hot melt adhesives; Wax blends; Industrial sealants.
Key Words:
Ethylene Vinyl Acetate; Exxon Chemical Company
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
0.947
g/cc
0.0342
lb/in³
Exxon Method
Apparent Bulk Density
0.540
g/cc
0.0195
lb/in³
ASTM D1895 (B)
Viscosity
300
cP
@Temperature 121 °C
300
cP
@Temperature 250 °F
melt viscosity; ASTM D-3236
Melt Flow
600
g/10 min
600
g/10 min
Exxon Method
Mechanical Properties
Metric
English
Comments
Hardness, Shore A
85
85
ASTM D2240
Tensile Strength, Ultimate
3.40
MPa
493
psi
ASTM D638
Elongation at Break
140 %
140 %
ASTM D638
Thermal Properties
Metric
English
Comments
Melting Point
78.0
°C
172
°F
Exxon Method
Ring & Ball Softening Point
89.0
°C
192
°F
ASTM E-28
**
Materials flagged as discontinued (
) are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.
Users of our Advanced Search (registration required) may exclude discontinued materials from search results.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Arkema EVATANE® 20-20 Copolymer Ethylene - Vinyl Acetate
Braskem Evateno® HM 728 EVA Hot Melt Copolymer
ExxonMobil Escorene™ UL 7511 Ethylene Vinyl Acetate Copolymer
ExxonMobil Escorene™ UL 7521 Ethylene Vinyl Acetate Copolymer
ExxonMobil Escorene® UL 7510 Adhesive Application Resin
PEXCEB / 37887
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.