MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Honeywell ETFE EX30 Mono-Axially Oriented, ETFE Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Fluoropolymer; ETFE/ECTFE; Fluorocarbon ETFE/ECTFE, Molded/Extruded; Nylon (Polyamide PA)

Material Notes: Description: ETFE EX30 is a 1.2 mil (30 micron) mono-axially oriented, ethylene tetrafluoroethylene (ETFE) film. It offers superior weather ability, UV transmission, chemical and graffiti resistance, exceptional clarity and enhanced mechanical properties. It is widely used as a protective film for long term outdoor applications like retro-reflective signage and photovoltaic cells.

Information provided by Honeywell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.183 g/cc1.183 g/ccASTM D1505
Density 1.77 g/cc0.0640 lb/in³Yield Density
Moisture Absorption at Equilibrium 0.0030 %0.0030 %ASTM D570
Water Vapor Transmission 12.92 g/m²/day
@Temperature 37.8 °C
0.8320 g/100 in²/day
@Temperature 100 °F
100%RH; ASTM F1249
Thickness 30.5 microns1.20 mil
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 70.3 - 82.0 MPa10200 - 11900 psiASTM D882
Film Tensile Strength at Yield, TD 24.1 - 41.4 MPa3500 - 6000 psiASTM D882
Film Elongation at Break, MD 130 - 160 %130 - 160 %ASTM D882
Film Elongation at Break, TD 390 - 520 %390 - 520 %ASTM D882
Film Elongation at Yield, MD 35 - 45 %35 - 45 %ASTM D882
Film Elongation at Yield, TD 15 - 17 %15 - 17 %ASTM D882
Secant Modulus, MD 1.338 - 1.53 GPa194.1 - 222 ksiASTM D882
Secant Modulus, TD 0.765 - 0.830 GPa111 - 120 ksiASTM D882
Coefficient of Friction 0.50 - 0.700.50 - 0.70film to stainless steel; ASTM D1894
 1.0 - 1.61.0 - 1.6film to film; ASTM D1894
Elmendorf Tear Strength, MD 32.8 - 39.4 g/micron833 - 1000 g/mil
Elmendorf Tear Strength, TD 45.94 - 52.48 g/micron1167 - 1333 g/milASTM D1922
Film Tensile Strength at Break, MD 100 - 134 MPa14500 - 19500 psiASTM D882
Film Tensile Strength at Break, TD 54.5 - 67.6 MPa7900 - 9800 psiASTM D882
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 2.6
@Frequency 1000 Hz
2.6
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 197 kV/mm5000 kV/inASTM D149(A)
 
Thermal PropertiesMetricEnglishComments
Melting Point 271 °C520 °FDTA
Oxygen Index 30 %30 %ASTM D2863
Shrinkage, MD  -7.00 %
@Treatment Temp. 150 °C,
Time 601 sec
-7.00 %
@Treatment Temp. 302 °F,
Time 0.167 hour
ASTM D1204
 -3.00 %
@Treatment Temp. 100 °C,
Time 601 sec
-3.00 %
@Treatment Temp. 212 °F,
Time 0.167 hour
ASTM D1204
Shrinkage, TD  1.0 %
@Treatment Temp. 100 °C,
Time 601 sec
1.0 %
@Treatment Temp. 212 °F,
Time 0.167 hour
ASTM D1204
 3.5 %
@Treatment Temp. 150 °C,
Time 601 sec
3.5 %
@Treatment Temp. 302 °F,
Time 0.167 hour
ASTM D1204
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.4071.407ASTM D542
Haze 1.5 - 4.5 %1.5 - 4.5 %ASTM D1003
Transmission, Visible 95 %95 %ASTM D1003

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Afton Plastics HT2183 Ethylene Tetrafluoroethylene
Solvay A6000 ETFE Fluoropolymer Film
Overview of materials for Polyimide
Overview of materials for Nylon 6, Film Grade
Overview of materials for Nylon 12, 50% Glass Fiber Filled

PALH02 / 23968

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.