Description: ETFE EX30 is a 1.2 mil (30 micron) mono-axially oriented, ethylene tetrafluoroethylene (ETFE) film. It offers superior weather ability, UV transmission, chemical and graffiti resistance, exceptional clarity and enhanced mechanical properties. It is widely used as a protective film for long term outdoor applications like retro-reflective signage and photovoltaic cells. Information provided by Honeywell. |