MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

FKuR Kunststoff Bio-Flex® F 1814 Compostable PLA Blend
Categories: Polymer; Film; Renewable/Recycled Polymer; Thermoplastic; Polylactic Acid (PLA) Biopolymer

Material Notes: Biodegradable and home compostable polymer compound suitable for blown film applications. Certified as home compostable according to EN 13432. Use in applications such as fruit bags.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.25 g/cc0.0452 lb/in³ISO 1183
Melt Flow 0.80 - 2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.80 - 2.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 29.0 MPa
@Thickness 0.0230 mm
4210 psi
@Thickness 0.000906 in
BUR 2.3; ISO 527-3
Film Tensile Strength at Yield, TD 28.0 MPa
@Thickness 0.0230 mm
4060 psi
@Thickness 0.000906 in
BUR 2.3; ISO 527-3
Film Elongation at Break, MD 600 %
@Thickness 0.0230 mm
600 %
@Thickness 0.000906 in
BUR 2.3; ISO 527-3
Film Elongation at Break, TD 370 %
@Thickness 0.0230 mm
370 %
@Thickness 0.000906 in
BUR 2.3; ISO 527-3
Elongation at Break 600 %600 %ISO 527-3
Tensile Modulus  0.130 GPa
@Thickness 0.0230 mm
18.9 ksi
@Thickness 0.000906 in
Film MD, BUR 2.3; ISO 527-3
 0.230 GPa
@Thickness 0.0230 mm
33.4 ksi
@Thickness 0.000906 in
Film TD, BUR 2.3; ISO 527-3
Elmendorf Tear Strength, MD 0.862 g/micron
@Thickness 0.0230 mm
21.9 g/mil
@Thickness 0.000906 in
BUR 2.3; ASTM D 1922
Elmendorf Tear Strength, TD 0.480 g/micron
@Thickness 0.0230 mm
12.2 g/mil
@Thickness 0.000906 in
BUR 2.3; ASTM D 1922
Film Tensile Strength at Break, MD 29.0 MPa
@Thickness 0.0230 mm
4210 psi
@Thickness 0.000906 in
BUR 2.3; ISO 527-3
Film Tensile Strength at Break, TD 28.0 MPa
@Thickness 0.0230 mm
4060 psi
@Thickness 0.000906 in
BUR 2.3; ISO 527-3
 
Thermal PropertiesMetricEnglishComments
Melting Point >= 155 °C>= 311 °FISO 3146-C
 
Descriptive Properties
Spencer Impact Test (N/mm)340ASTM D 3420, 23µm thickness, BUR 2.3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polylactic Acid (PLA) Biopolymer
FKuR Kunststoff Bio-Flex® F 1110 Compostable PLA Blend
FKuR Kunststoff Bio-Flex® F 1138 PLA Blend
FKuR Kunststoff Bio-Flex® F 7510 PLA Blend
GEHR Plastics ECO-GEHR® PLA-LF Polylactic Acid

PFKUR915 / 192740

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.