MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Elantas Conap FR-1050 Conapoxy® Resin / Conacure® Hardener
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Encapsulant, Unreinforced

Material Notes:
Epoxy Potting and Encapsulating Systems for Electronic Applications
High technology epoxy resin systems for potting and encapsulation, for the defense, aerospace, electronics, computer, automotive and related industries.

Cytec (Conap) FR-1050 Conapoxy® Resin / Conacure® Hardener
A low cost filled epoxy potting system. It has convenient 2 to 1 mix ratio and low viscosity.
  • Mix Ratio, Resin/Hardener (by weight): 100/50
Cure Type: Room Temperature

Information provided by Cytec, subsequently acquired by Elantas.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 6000 cP
@Temperature 25.0 °C
6000 cP
@Temperature 77.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8080
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 5.90e+15 ohm-cm<= 5.90e+15 ohm-cm
Dielectric Constant 2.83
@Frequency 1000 Hz
2.83
@Frequency 1000 Hz
Dielectric Strength 13.8 kV/mm350 kV/in
Dissipation Factor 0.011
@Frequency 1000 Hz
0.011
@Frequency 1000 Hz
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 110 °C230 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  960 min
@Temperature 60.0 °C
16.0 hour
@Temperature 140 °F
 4320 - 7200 min
@Temperature 25.0 °C
72.0 - 120 hour
@Temperature 77.0 °F
Pot Life 180 min180 min

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Elantas EN-2523 (Conap) Potting and Encapsulation Adhesive
Solvay BR® 680-3 Polyimide Film Adhesive
Solvay Thornel® T-650/35 3K Carbon Fiber, Polyacrylonitrile (PAN) Precursor
Solvay VTF 261 Film
Aurora Plastics GA-1050-OR3-LF PVC

PCYTEC38 / 29270

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.