System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Drill Down to All Materials Data Sheets
This series of pages is an inefficient set of links to all data sheets in MatWeb. We have several search tools, listed above, that give you more efficient methods to reach the information that you need.
Replacing...
Envalior Durethan® BKV 15 H2.0 901510 Nylon 6 (PA6), 15% Glass Fiber Reinforced, Dry
Envalior Durethan® BKV 15 H2.0 DUS008 901510 Nylon 6 (PA6), 15% Glass Fiber Reinforced, Conditioned
Envalior Durethan® BKV 15 H2.0 DUS008 901510 Nylon 6 (PA6), 15% Glass Fiber Reinforced, Dry
Envalior Durethan® BKV 15 H3.0 000000 Nylon 6 Copolymer, 15% Glass Fibers
Envalior Durethan® BKV 15 H3.0 DUS008 000000 Nylon 6 (PA6), 15% Glass Fiber Reinforced, Conditioned
Envalior Durethan® BKV 15 H3.0 DUS008 000000 Nylon 6 (PA6), 15% Glass Fiber Reinforced, Dry
Envalior Durethan® BKV 20 FN00 000000 Nylon 6, 18% Glass Fiber
Envalior Durethan® BKV 20 FN01 000000 Nylon 6 (PA6), 18% Glass Fiber Reinforced, Conditioned
Envalior Durethan® BKV 20 FN01 000000 Nylon 6 (PA6), 18% Glass Fiber Reinforced, Dry
Envalior Durethan® BKV 20 FN20 000000 Nylon 6 (PA6), 20% Glass Fiber Reinforced, Conditioned
Envalior Durethan® BKV 20 FN20 000000 Nylon 6 (PA6), 20% Glass Fiber Reinforced, Dry
Envalior Durethan® BKV 20 FN20 DUS013 000000 Nylon 6, 20% Glass Fiber
Envalior Durethan® BKV 215 000000 Nylon 6 (PA6), 15% Glass Fiber Reinforced, Conditioned
Envalior Durethan® BKV 215 000000 Nylon 6 (PA6), 15% Glass Fiber Reinforced, Dry
Envalior Durethan® BKV 215 901510 Copolyamide, 15% Glass Fiber
Envalior Durethan® BKV 215 H2.0 901510 Nylon 6 (PA6), 15% Glass Fiber Reinforced, Conditioned
Envalior Durethan® BKV 215 H2.0 901510 Nylon 6 (PA6), 15% Glass Fiber Reinforced, Dry
Envalior Durethan® BKV 215 H2.0 DUS008 901510 Nylon 6, Impact Modified
Envalior Durethan® BKV 215 H2.0 DUS035 900051 Nylon 6 (PA6), 15% Glass Fiber Reinforced, Conditioned
Envalior Durethan® BKV 215 H2.0 DUS035 900051 Nylon 6 (PA6), 15% Glass Fiber Reinforced, Dry
Envalior Durethan® BKV 215 H3.0 000000 Nylon 6 (PA6), 15% Glass Fiber Reinforced, Conditioned
Envalior Durethan® BKV 215 H3.0 000000 Nylon 6 (PA6), 15% Glass Fiber Reinforced, Dry
Envalior Durethan® BKV 215 W1 902176 Nylon 6 (PA6), 15% Glass Fiber Reinforced, Conditioned
Envalior Durethan® BKV 215 W1 902176 Nylon 6 (PA6), 15% Glass Fiber Reinforced, Dry
Envalior Durethan® BKV 230 000000 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Conditioned
Envalior Durethan® BKV 230 000000 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Dry
Envalior Durethan® BKV 230 DUS008 000000 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Conditioned
Envalior Durethan® BKV 230 DUS008 000000 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Dry
Envalior Durethan® BKV 230 H2.0 901510 Copolyamide, 30% Glass Fiber
Envalior Durethan® BKV 230 H2.0 DUS008 000000 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Conditioned
Envalior Durethan® BKV 230 H2.0 DUS008 000000 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Dry
Envalior Durethan® BKV 230 H3.0 000000 Nylon 6-Copolymer, 30% Glass Fibers
Envalior Durethan® BKV 240 H2.0 XCP 901510 Nylon 6 (PA6), 40% Glass Fiber Reinforced, Conditioned
Envalior Durethan® BKV 240 H2.0 XCP 901510 Nylon 6 (PA6), 40% Glass Fiber Reinforced, Dry
Envalior Durethan® BKV 25 F30 000000 Nylon 6 (PA6), 25% Glass Fiber Reinforced, Conditioned
Envalior Durethan® BKV 25 F30 000000 Nylon 6 (PA6), 25% Glass Fiber Reinforced, Dry
Envalior Durethan® BKV 25 FN01 000000 Nylon 6 (PA6), 25% Glass Fiber Reinforced, Conditioned
Envalior Durethan® BKV 25 FN01 000000 Nylon 6 (PA6), 25% Glass Fiber Reinforced, Dry
Envalior Durethan® BKV 25 FN27 000000 Nylon 6 (PA6), 25% Glass Fiber Reinforced, Conditioned
Envalior Durethan® BKV 25 FN27 000000 Nylon 6 (PA6), 25% Glass Fiber Reinforced, Dry
Envalior Durethan® BKV 25 H2.0 LT 904040 Nylon 6 (PA6), 25% Glass Fiber Reinforced, Conditioned
Envalior Durethan® BKV 25 H2.0 LT 904040 Nylon 6 (PA6), 25% Glass Fiber Reinforced, Dry
Envalior Durethan® BKV 30 000000 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Conditioned
Envalior Durethan® BKV 30 000000 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Dry
Envalior Durethan® BKV 30 DUS110 000000 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Conditioned
Envalior Durethan® BKV 30 DUS110 000000 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Dry
Envalior Durethan® BKV 30 EF 000000 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Conditioned
Envalior Durethan® BKV 30 EF 000000 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Dry
Envalior Durethan® BKV 30 FN00 000000 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Conditioned
Envalior Durethan® BKV 30 FN00 000000 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Dry
Envalior Durethan® BKV 30 G H2.0 900051 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Conditioned
Envalior Durethan® BKV 30 G H2.0 900051 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Dry
Envalior Durethan® BKV 30 G H2.0 900116 Nylon 6, 30% Glass Fiber
Envalior Durethan® BKV 30 G W1 901317 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Conditioned
Envalior Durethan® BKV 30 G W1 901317 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Dry
Envalior Durethan® BKV 30 H2.0 000000 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Conditioned
Envalior Durethan® BKV 30 H2.0 000000 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Dry
Envalior Durethan® BKV 30 H2.0 901510 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Conditioned
Envalior Durethan® BKV 30 H2.0 901510 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Dry
Envalior Durethan® BKV 30 H2.0 EF 000000 Nylon 6, Glass Fiber Reinforced
Envalior Durethan® BKV 30 H2.0 EF 900116 Nylon 6, 30% Glass Fiber
Envalior Durethan® BKV 30 H2.0 EF 901510 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Conditioned
Envalior Durethan® BKV 30 H2.0 EF 901510 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Dry
Envalior Durethan® BKV 30 H2.0 EF DUS029 901510 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Conditioned
Envalior Durethan® BKV 30 H2.0 EF DUS029 901510 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Dry
Envalior Durethan® BKV 30 H3.0 000000 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Conditioned
Envalior Durethan® BKV 30 H3.0 000000 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Dry
Envalior Durethan® BKV 30 HTS 901510 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Conditioned
Envalior Durethan® BKV 30 HTS 901510 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Dry
Envalior Durethan® BKV 30 N1 000000 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Conditioned
Envalior Durethan® BKV 30 N1 000000 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Dry
Envalior Durethan® BKV 30 W1 000000 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Conditioned
Envalior Durethan® BKV 30 W1 000000 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Dry
Envalior Durethan® BKV 30 XTS1 901510 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Conditioned
Envalior Durethan® BKV 30 XTS1 901510 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Dry
Envalior Durethan® BKV 315 Z H2.0 901510 Nylon 6 (PA6), 15% Glass Fiber Reinforced, Conditioned
Envalior Durethan® BKV 315 Z H2.0 901510 Nylon 6 (PA6), 15% Glass Fiber Reinforced, Dry
Envalior Durethan® BKV 325 Z H2.0 901510 Nylon 6 (PA6), 25% Glass Fiber Reinforced, Conditioned
Envalior Durethan® BKV 325 Z H2.0 901510 Nylon 6 (PA6), 25% Glass Fiber Reinforced, Dry
Envalior Durethan® BKV 330 H2.0 901510 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Conditioned
Envalior Durethan® BKV 330 H2.0 901510 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Dry
Envalior Durethan® BKV 35 000000 Nylon 6 (PA6), 35% Glass Fiber Reinforced, Conditioned
Envalior Durethan® BKV 35 000000 Nylon 6 (PA6), 35% Glass Fiber Reinforced, Dry
Envalior Durethan® BKV 35 CX H2.0 900876 Nylon 6 (PA6), 35% Glass Fiber Reinforced, Conditioned
Envalior Durethan® BKV 35 CX H2.0 900876 Nylon 6 (PA6), 35% Glass Fiber Reinforced, Dry
Envalior Durethan® BKV 35 H2.0 901510 Nylon 6 (PA6), 35% Glass Fiber Reinforced, Conditioned
Envalior Durethan® BKV 35 H2.0 901510 Nylon 6 (PA6), 35% Glass Fiber Reinforced, Dry
Envalior Durethan® BKV 35 H2.0 EF 900116 Nylon 6 (PA6), 35% Glass Fiber Reinforced, Conditioned
Envalior Durethan® BKV 35 H2.0 EF 900116 Nylon 6 (PA6), 35% Glass Fiber Reinforced, Dry
Envalior Durethan® BKV 35 H2.0 EF 901510 Nylon 6 (PA6), 35% Glass Fiber Reinforced, Conditioned
Envalior Durethan® BKV 35 H2.0 EF 901510 Nylon 6 (PA6), 35% Glass Fiber Reinforced, Dry
Envalior Durethan® BKV 35 H3.0 000000 Nylon 6, Glass Fiber Reinforced
Envalior Durethan® BKV 35 HTS 901510 Nylon 6 (PA6), 35% Glass Fiber Reinforced, Conditioned
Envalior Durethan® BKV 35 HTS 901510 Nylon 6 (PA6), 35% Glass Fiber Reinforced, Dry
Envalior Durethan® BKV 35 XTS1 901510 Nylon 6 (PA6), 35% Glass Fiber Reinforced, Conditioned
Envalior Durethan® BKV 35 XTS1 901510 Nylon 6 (PA6), 35% Glass Fiber Reinforced, Dry
Envalior Durethan® BKV 40 H2.0 901510 Nylon 6 (PA6), 40% Glass Fiber Reinforced, Conditioned
Envalior Durethan® BKV 40 H2.0 901510 Nylon 6 (PA6), 40% Glass Fiber Reinforced, Dry
Envalior Durethan® BKV 40 H3.0 000000 Nylon 6 (PA6), 40% Glass Fiber Reinforced, Conditioned
Envalior Durethan® BKV 40 H3.0 000000 Nylon 6 (PA6), 40% Glass Fiber Reinforced, Dry
Envalior Durethan® BKV 40H2.0 EF 900116 Nylon 6, Glass Fiber Reinforced
Envalior Durethan® BKV 50 000000 Nylon 6 (PA6), 50% Glass Fiber Reinforced, Conditioned
Envalior Durethan® BKV 50 000000 Nylon 6 (PA6), 50% Glass Fiber Reinforced, Dry
Envalior Durethan® BKV 50 G H2.0 EF 000000 Nylon 6 (PA6), 50% Glass Fiber Reinforced, Conditioned
Envalior Durethan® BKV 50 G H2.0 EF 000000 Nylon 6 (PA6), 50% Glass Fiber Reinforced, Dry
Envalior Durethan® BKV 50 H EF DUS022 900116 Nylon 6, Glass Fiber Reinforced
Envalior Durethan® BKV 50 H2.0 901510 Nylon 6 (PA6), 50% Glass Fiber Reinforced, Conditioned
Envalior Durethan® BKV 50 H2.0 901510 Nylon 6 (PA6), 50% Glass Fiber Reinforced, Dry
Envalior Durethan® BKV 50 H2.0 EF 000000 Nylon 6, 50% Glass Fiber
Envalior Durethan® BKV 50 H2.0 EF 900116 Nylon 6 (PA6), 50% Glass Fiber Reinforced, Conditioned
Envalior Durethan® BKV 50 H2.0 EF 900116 Nylon 6 (PA6), 50% Glass Fiber Reinforced, Dry
Envalior Durethan® BKV 50 H2.0 EF DUS030 901510 Nylon 6 (PA6), 50% Glass Fiber Reinforced, Conditioned
Envalior Durethan® BKV 50 H2.0 EF DUS030 901510 Nylon 6 (PA6), 50% Glass Fiber Reinforced, Dry
Envalior Durethan® BKV 50 H3.0 000000 Nylon 6 (PA6), 50% Glass Fiber Reinforced, Conditioned
Envalior Durethan® BKV 50 H3.0 000000 Nylon 6 (PA6), 50% Glass Fiber Reinforced, Dry
Envalior Durethan® BKV 55 TPX 900116 Nylon 6 (PA6), 55% Glass Fiber Reinforced, Conditioned
Envalior Durethan® BKV 55 TPX 900116 Nylon 6 (PA6), 55% Glass Fiber Reinforced, Dry
Envalior Durethan® BKV 60 EF DUS097 000000 Nylon 6 (PA6), 60% Glass Fiber Reinforced, Conditioned
Envalior Durethan® BKV 60 EF DUS097 000000 Nylon 6 (PA6), 60% Glass Fiber Reinforced, Dry
Envalior Durethan® BKV 60 H2.0 EF DUS060 900116 Nylon 6 (PA6), 60% Glass Fiber Reinforced, Conditioned
Envalior Durethan® BKV 60 H2.0 EF DUS060 900116 Nylon 6 (PA6), 60% Glass Fiber Reinforced, Dry
Envalior Durethan® BKV 60 H3.0 EF 900116 Nylon 6 (PA6), 60% Glass Fiber Reinforced, Conditioned
Envalior Durethan® BKV 60 H3.0 EF 900116 Nylon 6 (PA6), 60% Glass Fiber Reinforced, Dry
Envalior Durethan® BKV 60 XF 900116 Nylon 6 (PA6), 60% Glass Fiber Reinforced, Conditioned
Envalior Durethan® BKV 60 XF 900116 Nylon 6 (PA6), 60% Glass Fiber Reinforced, Dry
Envalior Durethan® BKY 115 H3.0 DUS008 Nylon 6, 15% Glass Fiber
Envalior Durethan® BM 130 H2.0 901510 Nylon 6 (PA6), 30% Mineral Reinforced, Conditioned
Envalior Durethan® BM 130 H2.0 901510 Nylon 6 (PA6), 30% Mineral Reinforced, Dry
Envalior Durethan® BM 230 H2.0 901510 Nylon 6 (PA6), 30% Mineral Filled, Conditioned
Envalior Durethan® BM 230 H2.0 901510 Nylon 6 (PA6), 30% Mineral Filled, Dry
Envalior Durethan® BM 240 000000 Nylon 6 (PA6), 40% Mineral Filled, Conditioned
Envalior Durethan® BM 240 000000 Nylon 6 (PA6), 40% Mineral Filled, Dry
Envalior Durethan® BM 240 H2.0 901510 Nylon 6 (PA6), 40% Mineral Filled, Conditioned
Envalior Durethan® BM 240 H2.0 901510 Nylon 6 (PA6), 40% Mineral Filled, Dry
Envalior Durethan® BM 240 H3.0 000000 Nylon 6 (PA6), 40% Mineral Filled, Conditioned
Envalior Durethan® BM 240 H3.0 000000 Nylon 6 (PA6), 40% Mineral Filled, Dry
Envalior Durethan® BM 25 FN20 700350 Nylon 6 (PA6), 25% Mineral Filled, Conditioned
Envalior Durethan® BM 25 FN20 700350 Nylon 6 (PA6), 25% Mineral Filled, Dry
Envalior Durethan® BM 25 FN20 DUS013 000000 Nylon 6 (PA6), 25% Mineral Filled, Conditioned
Envalior Durethan® BM 25 FN20 DUS013 000000 Nylon 6 (PA6), 25% Mineral Filled, Dry
Envalior Durethan® BM 29 X H1.0 000000 Nylon 6 (PA6), 30% Glass/Mineral Reinforced, Conditioned
Envalior Durethan® BM 29 X H1.0 000000 Nylon 6 (PA6), 30% Glass/Mineral Reinforced, Dry
Envalior Durethan® BM 29 X H2.0 EF 900116 Nylon 6 (PA6), 30% Glass/Mineral Filled, Conditioned
Envalior Durethan® BM 29 X H2.0 EF 900116 Nylon 6 (PA6), 30% Glass/Mineral Filled, Dry
Envalior Durethan® BM 40 X H2.0 DUS009 901510 Nylon 6 (PA6), 40% Glass/Mineral Reinforced, Conditioned
Envalior Durethan® BM 40 X H2.0 DUS009 901510 Nylon 6 (PA6), 40% Glass/Mineral Reinforced, Dry
Envalior Durethan® BM 40 X H2.0 EF 900116 Nylon 6 (PA6), 40% Glass/Mineral Filled, Conditioned
Envalior Durethan® BM 40 X H2.0 EF 900116 Nylon 6 (PA6), 40% Glass/Mineral Filled, Dry
Envalior Durethan® BM 40 X H3.0 EF 000000 Nylon 6 (PA6), 40% Glass/Mineral Filled, Conditioned
Envalior Durethan® BM 40 X H3.0 EF 000000 Nylon 6 (PA6), 40% Glass/Mineral Filled, Dry
Envalior Durethan® BM 430 H2.0 901510 Nylon 6 (PA6), 30% Mineral Filled, Conditioned
Envalior Durethan® BM 430 H2.0 901510 Nylon 6 (PA6), 30% Mineral Filled, Dry
Envalior Durethan® BTC 65 H3.0 EF 901510 Nylon 6 (PA6), 65% Mineral Filled, Conditioned
Envalior Durethan® BTC 65 H3.0 EF 901510 Nylon 6 (PA6), 65% Mineral Filled, Dry
Envalior Durethan® C 38 F 000000 Nylon 6 (PA6), Conditioned
Envalior Durethan® C 38 F 000000 Nylon 6 (PA6), Dry
Envalior Durethan® C 38 FA 000000 Nylon 6 (PA6), Conditioned
Envalior Durethan® C 38 FA 000000 Nylon 6 (PA6), Dry
Envalior Durethan® C 38 FAM 000000 Copolyamide
Envalior Durethan® C 38 FAM 000000 Nylon 6 (PA6), Conditioned
Envalior Durethan® C 38 FAM 000000 Nylon 6 (PA6), Dry
Envalior Durethan® C 38 FKAM 000000 Nylon 6 (PA6), Conditioned
Envalior Durethan® C 38 FKAM 000000 Nylon 6 (PA6), Dry
Envalior Durethan® C 38 FKS 000000 Copolyamide
Envalior Durethan® CI 31 F 000000 Copolyamide PA6/6I
Envalior Durethan® CPA 31 000000 Nylon 6 (PA6)/66, Dry
Envalior Durethan® CPA 31 000000 Nylon 6 (PA6)/66,Conditioned
Envalior Durethan® DP 1100/30 H2.0 901510 Nylon 6 (PA6), 30% Micro bead Reinforced, Conditioned
Envalior Durethan® DP 1100/30 H2.0 901510 Nylon 6 (PA6), 30% Micro bead Reinforced, Dry
Envalior Durethan® DP 1336 901510 Nylon 6 (PA6), Conditioned
Envalior Durethan® DP 1336 901510 Nylon 6 (PA6), Dry
Envalior Durethan® DP 1441/40 H2.0 EF 900116 Nylon 6 (PA6), 40% Glass/Mineral Reinforced, Conditioned
Envalior Durethan® DP 1441/40 H2.0 EF 900116 Nylon 6 (PA6), 40% Glass/Mineral Reinforced, Dry
Envalior Durethan® DP 1801/30 H3.0 000000 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Flame Retardant, Conditioned
Envalior Durethan® DP 1801/30 H3.0 000000 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Flame Retardant, Dry
Envalior Durethan® DP 1802 H3.0 000000 Nylon 6 (PA6), Dry
Envalior Durethan® DP 1802 H3.0 000000 Nylon 6 (PA6),Conditioned
Envalior Durethan® DP 1803/10 H3.0 000000 Nylon 6 (PA6), 50% Glass/Mineral Reinforced, Flame Retardant, Conditioned
Envalior Durethan® DP 1803/10 H3.0 000000 Nylon 6 (PA6), 50% Glass/Mineral Reinforced, Flame Retardant, Dry
Envalior Durethan® DP 1852/30 000000 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Flame Retardant, Conditioned
Envalior Durethan® DP 1852/30 000000 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Flame Retardant, Dry
Envalior Durethan® DP 2037/30 H2.0 LT 904040 Nylon 6, 30% Glass Fiber
Envalior Durethan® DP 2131/20 H2.0 900051 Nylon 6 (PA6), 20% Glass Fiber Reinforced, Conditioned
Envalior Durethan® DP 2131/20 H2.0 900051 Nylon 6 (PA6), 20% Glass Fiber Reinforced, Dry
Envalior Durethan® DP 2131/20 H3.0 000000 Nylon 6 (PA6), 20% Glass Fiber Reinforced, Conditioned
Envalior Durethan® DP 2131/20 H3.0 000000 Nylon 6 (PA6), 20% Glass Fiber Reinforced, Dry
Envalior Durethan® DP 2131/20 W1 901317 Nylon 6 (PA6), 20% Glass Fiber Reinforced, Conditioned
Envalior Durethan® DP 2131/20 W1 901317 Nylon 6 (PA6), 20% Glass Fiber Reinforced, Dry
Envalior Durethan® DP 2-2224/30 H2.0 901510 Nylon 6 (PA6), 30% Glass/Mineral Reinforced, Conditioned
Envalior Durethan® DP 2-2224/30 H2.0 901510 Nylon 6 (PA6), 30% Glass/Mineral Reinforced, Dry
Envalior Durethan® DP 2-2240/15 H2.0 901510 Nylon 66 (PA66), 15% Glass Fiber Reinforced, Conditioned
Envalior Durethan® DP 2-2240/15 H2.0 901510 Nylon 66 (PA66), 15% Glass Fiber Reinforced, Dry
Envalior Durethan® DP 2325 H3.0 000000 Nylon 66 (PA66), Conditioned
Envalior Durethan® DP 2325 H3.0 000000 Nylon 66 (PA66), Dry
Envalior Durethan® DP 2325 H3.0 DUS031 000000 Nylon 66
Envalior Durethan® DP 2801 000000 Nylon 66 (PA66), Conditioned
Envalior Durethan® DP 2801 000000 Nylon 66 (PA66), Dry
Envalior Durethan® DP 2802/30 000000 Nylon 66 (PA66), 30% Glass Fiber Reinforced, Conditioned
Envalior Durethan® DP 2802/30 000000 Nylon 66 (PA66), 30% Glass Fiber Reinforced, Dry
Envalior Durethan® DP 2851/30 H3.0 000000 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Flame Retardant, Conditioned
Envalior Durethan® DP 2851/30 H3.0 000000 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Flame Retardant, Dry
Envalior Durethan® DP A 30 S FN30 DUS025 000000 Nylon 66
Envalior Durethan® DP A 32 901510 Nylon 66
Envalior Durethan® DP AKV 30 FN00 000000 Nylon 66 (PA66), 30% Glass Fiber Reinforced, Conditioned
Envalior Durethan® DP AKV 30 FN00 000000 Nylon 66 (PA66), 30% Glass Fiber Reinforced, Dry
Envalior Durethan® DP AKV 30 FN00 DUS013 000000 Nylon 66 (PA66), 30% Glass Fiber Reinforced, Conditioned
Envalior Durethan® DP AKV 30 FN00 DUS013 000000 Nylon 66 (PA66), 30% Glass Fiber Reinforced, Dry
Envalior Durethan® DP AKV 30 FN00 DUS013 Nylon 66, 30% Glass Fiber
Envalior Durethan® DP AKV 30 HR EF 901510 Nylon 66 (PA66), 30% Glass Fiber Reinforced, Conditioned
Envalior Durethan® DP AKV 30 HR EF 901510 Nylon 66 (PA66), 30% Glass Fiber Reinforced, Dry
Envalior Durethan® DP AKV 30 X HR 900116 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Dry
Envalior Durethan® DP AKV 30 X HR EF 900116 Nylon 66, 30% Glass Fiber
Envalior Durethan® DP AKV 35 LT H2.0 904040 Nylon 66, 35% Glass Fiber
Envalior Durethan® DP AKV 50 HR H2.0 901510 Nylon 66 (PA66), 50% Glass Fiber Reinforced, Conditioned
Envalior Durethan® DP AKV 50 HR H2.0 901510 Nylon 66 (PA66), 50% Glass Fiber Reinforced, Dry
Envalior Durethan® DP BC 310 EF 000000 Nylon 6
Envalior Durethan® DP BC 310 EF 600065 Nylon 6
Envalior Durethan® DP BC 500 H2.0 901510 Nylon 6 (PA6), Conditioned
Envalior Durethan® DP BC 500 H2.0 901510 Nylon 6 (PA6), Dry
Envalior Durethan® DP BC 600 HTS 900116 Nylon 6 (PA6), Conditioned
Envalior Durethan® DP BC 600 HTS 900116 Nylon 6 (PA6), Dry
Envalior Durethan® DP BKV 240 H2.0 901510 Nylon 6 (PA6), 40% Glass Fiber Reinforced, Conditioned
Envalior Durethan® DP BKV 240 H2.0 901510 Nylon 6 (PA6), 40% Glass Fiber Reinforced, Dry
Envalior Durethan® DP BKV 30 XF 000000 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Conditioned
Envalior Durethan® DP BKV 30 XF 000000 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Dry
Envalior Durethan® DP BKV 35 XF 901510 Nylon 6 (PA6), 35% Glass Fiber Reinforced, Conditioned
Envalior Durethan® DP BKV 35 XF 901510 Nylon 6 (PA6), 35% Glass Fiber Reinforced, Dry
Envalior Durethan® DP BKV 60 EF 000000 Nylon6, 60% Glass Fiber
Envalior Durethan® DP BKV 60 H2.0 EF 900116 Nylon 6 (PA6), 60% Glass Fiber Reinforced, Conditioned
Envalior Durethan® DP BKV 60 H2.0 EF 900116 Nylon 6 (PA6), 60% Glass Fiber Reinforced, Dry
Envalior Durethan® DP BM 29 X H2.0 EF 900116 Nylon 6 (PA6), 30% Glass/Mineral Reinforced, Conditioned
Envalior Durethan® DP BM 29 X H2.0 EF 900116 Nylon 6 (PA6), 30% Glass/Mineral Reinforced, Dry
Envalior Durethan® DP BM 410 H2.0 901510 Nylon 6, 10% Mineral + Glass Fiber
Envalior Durethan® DP BM 65 X FM30 901510 Nylon 6 (PA6), 65% Mineral/Glass Fiber Reinforced, Conditioned
Envalior Durethan® DP BM 65 X FM30 901510 Nylon 6 (PA6), 65% Mineral/Glass Fiber Reinforced, Dry
Envalior Durethan® ECO BKV 20 FN20 000000 Nylon 6 (PA6), 20% Glass Fiber Reinforced, Conditioned
Envalior Durethan® ECO BKV 20 FN20 000000 Nylon 6 (PA6), 20% Glass Fiber Reinforced, Dry
Envalior Durethan® ECO BV 30 H2 900500 Nylon 6, 30% Glass Fiber
Envalior Durethan® ECO BV 35 H2 900500 Nylon 6, 35% Glass Fiber
Envalior Durethan® ECO PA GF30 909040 Nylon 6, 30% Glass Fiber
Envalior Durethan® KL 1-2218/40 H2.0 901510 Nylon 6 (PA6), 40% Glass/Mineral Reinforced, Conditioned
Envalior Durethan® KL 1-2218/40 H2.0 901510 Nylon 6 (PA6), 40% Glass/Mineral Reinforced, Dry
Envalior Durethan® KL 1-2403/40 H1.0 000000 Nylon 6 (PA6), 40% Mineral Reinforced, Conditioned
Envalior Durethan® KL 1-2403/40 H1.0 000000 Nylon 6 (PA6), 40% Mineral Reinforced, Dry
Envalior Durethan® KU 2-2183 000000 Nylon 6 (PA6), Flame Retardant, Conditioned
Envalior Durethan® KU 2-2183 000000 Nylon 6 (PA6), Flame Retardant, Dry
Envalior Durethan® KU 2-2184/15 H3.0 000000 Nylon 6 (PA6), 65% Glass/Mineral Reinforced, Flame Retardant, Conditioned
Envalior Durethan® KU 2-2184/15 H3.0 000000 Nylon 6 (PA6), 65% Glass/Mineral Reinforced, Flame Retardant, Dry
Envalior Durethan® T 40 000000 Partially aromatic polyamide
Envalior Durethan® T 40 ZS 000000 Partially aromatic polyamide
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.