MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Envalior Durethan® BKV 35 H3.0 000000 Nylon 6, Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 40% Glass Fiber Filled

Material Notes: PA 6, 35% glass fibers, injection molding, heat-aging stabilized

Former Lanxess product line is now with Envalior.

Vendors:
Available Properties
  • Specific Gravity, ISO 1183
  • Moisture Absorption at Equilibrium, ISO 62, 50% RH
  • Water Absorption at Saturation, ISO 62
  • Linear Mold Shrinkage, Flow, ISO 2577, Post-shrinkage, 150x105x3; 120°C; 4 hour
  • Linear Mold Shrinkage, Flow, ISO 294-4, Post-shrinkage, 60x60x2; 120°C; 4 hour
  • Linear Mold Shrinkage, Flow, ISO 2577, 150x105x3; 280°C / MT 80°C; 500 bar
  • Linear Mold Shrinkage, Flow, ISO 294-4, 60x60x2; 280°C / MT 80°C; 600 bar
  • Linear Mold Shrinkage, Transverse, ISO 294-4, Post-shrinkage, 60x60x2; 120°C; 4 hour
  • Linear Mold Shrinkage, Transverse, ISO 2577, Post-shrinkage, 150x105x3; 120°C; 4 hour
  • Linear Mold Shrinkage, Transverse, ISO 294-4, 60x60x2; 280°C / MT 80°C; 600 bar
  • Linear Mold Shrinkage, Transverse, ISO 2577, 150x105x3; 280°C / MT 80°C; 500 bar
  • Tensile Strength at Break, ISO 527-1, -2; 5 mm/min, cond.
  • Tensile Strength at Break, ISO 527-1, -2; 5 mm/min, d.a.m.
  • Elongation at Break, ISO 527-1, -2; 5 mm/min, d.a.m.
  • Elongation at Break, ISO 527-1, -2; 5 mm/min, cond.
  • Tensile Modulus, ISO 527-1, -2; 1 mm/min, cond.
  • Tensile Modulus, ISO 527-1, -2; 1 mm/min, d.a.m.
  • Flexural Strength, ISO 178-A, cond., 2 mm/min
  • Flexural Strength, ISO 178-A, d.a.m., 2 mm/min
  • Flexural Yield Strength, ISO 178-A, cond., 2 mm/min
  • Flexural Modulus, ISO 178-A, cond., 2 mm/min
  • Flexural Modulus, ISO 178-A, d.a.m., 2 mm/min
  • Izod Impact, Notched (ISO), ISO 180-1A, d.a.m.
  • Izod Impact, Notched (ISO), ISO 180-1A, cond.
  • Izod Impact, Notched (ISO), ISO 180-1A, d.a.m.
  • Izod Impact, Notched (ISO), ISO 180-1A, cond.
  • Izod Impact, Unnotched (ISO), ISO 180-1U, d.a.m.
  • Charpy Impact Unnotched, ISO 179-1eU, d.a.m.
  • Charpy Impact Unnotched, ISO 179-1eU, cond.
  • Charpy Impact Unnotched, ISO 179-1eU, d.a.m.
  • Charpy Impact Unnotched, ISO 179-1eU, cond.
  • Charpy Impact, Notched, ISO 179-1eA, d.a.m.
  • Charpy Impact, Notched, ISO 179-1eA, cond.
  • Charpy Impact, Notched, ISO 179-1eA, d.a.m.
  • Charpy Impact, Notched, ISO 179-1eA, cond.
  • Tensile Creep Modulus, 1 hour, ISO 899-1, cond.
  • Tensile Creep Modulus, 1000 hours, ISO 899-1, cond.
  • Volume Resistivity, IEC 60093, cond.
  • Volume Resistivity, IEC 60093, d.a.m.
  • Surface Resistance, IEC 60093, cond.
  • Surface Resistance, IEC 60093, d.a.m.
  • Dielectric Constant, IEC 60250, d.a.m.
  • Dielectric Constant, IEC 60250, d.a.m.
  • Dielectric Constant, IEC 60250, cond.
  • Dielectric Constant, IEC 60250, cond.
  • Dielectric Strength, IEC 60243-1, cond.
  • Dielectric Strength, IEC 60243-1, d.a.m.
  • Dissipation Factor, IEC 60250, d.a.m.
  • Dissipation Factor, IEC 60250, d.a.m.
  • Dissipation Factor, IEC 60250, cond.
  • Dissipation Factor, IEC 60250, cond.
  • Comparative Tracking Index, IEC 60112, d.a.m.; Solution A
  • CTE, linear, Parallel to Flow, ISO 11359-1, -2
  • CTE, linear, Transverse to Flow, ISO 11359-1, -2
  • Melting Point, ISO 11357-1, -3, 10°C/min
  • Deflection Temperature at 0.46 MPa (66 psi), ISO 75-1, -2
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75-1, -2
  • Vicat Softening Point, ISO 306, 120°C/hour
  • Flammability, UL94
  • Flammability, UL94
  • Glow Wire Flammability Index, IEC 60695-2-12
  • Melt Temperature
  • Melt Temperature, ISO 294, for test specimens
  • Mold Temperature, ISO 294, for test specimens
  • Mold Temperature
  • Drying Temperature
  • Dry Time
  • Moisture Content, Karl Fischer Test, residual
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Envalior, former LANXESS

Category Notes
Plastic
PA, Polyamide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.