MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Acetal Copolymer, Impact Modified
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Impact Modified

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Impact Modified". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.07 - 1.41 g/cc0.0387 - 0.0509 lb/in³Average value: 1.35 g/cc Grade Count:116
 1.14 - 1.14 g/cc
@Temperature 205 - 205 °C
0.0412 - 0.0412 lb/in³
@Temperature 401 - 401 °F
Average value: 1.14 g/cc Grade Count:2
Water Absorption 0.200 - 1.10 %0.200 - 1.10 %Average value: 0.418 % Grade Count:32
Moisture Absorption at Equilibrium 0.200 - 0.350 %0.200 - 0.350 %Average value: 0.237 % Grade Count:16
Water Absorption at Saturation 0.650 - 1.20 %0.650 - 1.20 %Average value: 0.868 % Grade Count:38
Maximum Moisture Content 0.1500.150Average value: 0.150 Grade Count:5
 0.200 - 0.200
@Temperature 100 - 100 °C
0.200 - 0.200
@Temperature 212 - 212 °F
Average value: 0.200 Grade Count:2
 0.200 - 0.200
@Time 299 - 299 sec
0.200 - 0.200
@Time 0.0830 - 0.0830 hour
Average value: 0.200 Grade Count:2
Linear Mold Shrinkage 0.00700 - 0.0350 cm/cm0.00700 - 0.0350 in/inAverage value: 0.0179 cm/cm Grade Count:78
Linear Mold Shrinkage, Transverse 0.00800 - 0.0210 cm/cm0.00800 - 0.0210 in/inAverage value: 0.0163 cm/cm Grade Count:43
Melt Flow 0.600 - 27.8 g/10 min0.600 - 27.8 g/10 minAverage value: 7.99 g/10 min Grade Count:80
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 18.7 - 78.018.7 - 78.0Average value: 58.0 Grade Count:15
Hardness, Rockwell R 75.0 - 11675.0 - 116Average value: 99.6 Grade Count:12
Ball Indentation Hardness 35.0 - 120 MPa5080 - 17400 psiAverage value: 88.6 MPa Grade Count:14
Tensile Strength, Ultimate 26.0 - 56.0 MPa3770 - 8120 psiAverage value: 40.6 MPa Grade Count:38
Tensile Strength, Yield 23.0 - 68.9 MPa3340 - 10000 psiAverage value: 44.3 MPa Grade Count:77
 22.0 - 80.0 MPa
@Temperature -40.0 - 80.0 °C
3190 - 11600 psi
@Temperature -40.0 - 176 °F
Average value: 51.0 MPa Grade Count:2
Elongation at Break 10.0 - 300 %10.0 - 300 %Average value: 73.1 % Grade Count:89
Elongation at Yield 6.00 - 85.0 %6.00 - 85.0 %Average value: 14.8 % Grade Count:64
 7.50 - 17.0 %
@Temperature -40.0 - 80.0 °C
7.50 - 17.0 %
@Temperature -40.0 - 176 °F
Average value: 12.3 % Grade Count:2
Modulus of Elasticity 0.772 - 2.45 GPa112 - 355 ksiAverage value: 1.70 GPa Grade Count:73
Flexural Yield Strength 24.0 - 107 MPa3480 - 15500 psiAverage value: 50.9 MPa Grade Count:53
Flexural Modulus 0.750 - 3.14 GPa109 - 455 ksiAverage value: 1.65 GPa Grade Count:92
Poissons Ratio 0.430 - 0.4400.430 - 0.440Average value: 0.433 Grade Count:3
Izod Impact, Notched 0.490 - 100 J/cm0.918 - 187 ft-lb/inAverage value: 1.20 J/cm Grade Count:21
 0.590 - 0.907 J/cm
@Temperature -40.0 - -30.0 °C
1.11 - 1.70 ft-lb/in
@Temperature -40.0 - -22.0 °F
Average value: 0.849 J/cm Grade Count:4
 1.03 - 1.03 J/cm
@Temperature -30.0 - -30.0 °C
1.93 - 1.93 ft-lb/in
@Temperature -22.0 - -22.0 °F
Average value: 0.849 J/cm Grade Count:1
 1.03 - 1.03 J/cm
@Thickness 6.40 - 6.40 mm
1.93 - 1.93 ft-lb/in
@Thickness 0.252 - 0.252 in
Average value: 0.849 J/cm Grade Count:1
Izod Impact, Notched (ISO) 7.00 - 90.0 kJ/m²3.33 - 42.8 ft-lb/in²Average value: 17.1 kJ/m² Grade Count:19
 14.0 - 20.0 kJ/m²
@Temperature -40.0 - -30.0 °C
6.66 - 9.52 ft-lb/in²
@Temperature -40.0 - -22.0 °F
Average value: 17.0 kJ/m² Grade Count:2
Charpy Impact Unnotched 6.00 J/cm² - NB28.6 ft-lb/in² - NBAverage value: 14.6 J/cm² Grade Count:56
 -4.62 J/cm² - NB
@Temperature -30.0 - -30.0 °C
-22.0 ft-lb/in² - NB
@Temperature -22.0 - -22.0 °F
Average value: 16.9 J/cm² Grade Count:44
Charpy Impact, Notched 0.500 J/cm² - NB2.38 ft-lb/in² - NBAverage value: 1.97 J/cm² Grade Count:90
 0.504 - 1.806 J/cm²
@Temperature -30.0 - -30.0 °C
2.40 - 8.595 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 0.935 J/cm² Grade Count:49
Coefficient of Friction 0.400 - 0.5000.400 - 0.500Average value: 0.483 Grade Count:3
Penetration 5.00 - 55.05.00 - 55.0Average value: 21.0 Grade Count:7
Tensile Creep Modulus, 1 hour 700 - 1850 MPa102000 - 268000 psiAverage value: 1470 MPa Grade Count:24
Tensile Creep Modulus, 1000 hours 400 - 1050 MPa58000 - 152000 psiAverage value: 839 MPa Grade Count:24
K (wear) Factor 1.00 - 600 x 10-8 mm³/N-M0.496 - 298 x 10-10 in³-min/ft-lb-hrAverage value: 213 x 10-8 mm³/N-M Grade Count:3
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 10000 - 1.00e+16 ohm-cm10000 - 1.00e+16 ohm-cmAverage value: 1.48e+15 ohm-cm Grade Count:57
Surface Resistance 260 - 1.00e+16 ohm260 - 1.00e+16 ohmAverage value: 2.13e+15 ohm Grade Count:57
Dielectric Constant 3.40 - 5.303.40 - 5.30Average value: 4.06 Grade Count:39
Dielectric Strength 17.7 - 86.6 kV/mm450 - 2200 kV/inAverage value: 30.8 kV/mm Grade Count:34
Dissipation Factor 0.000600 - 0.04250.000600 - 0.0425Average value: 0.0116 Grade Count:35
Comparative Tracking Index 600 V600 VAverage value: 600 V Grade Count:30
 
Thermal PropertiesMetricEnglishComments
CTE, linear 70.0 - 142 µm/m-°C38.9 - 78.9 µin/in-°FAverage value: 123 µm/m-°C Grade Count:69
CTE, linear, Transverse to Flow 110 - 180 µm/m-°C61.1 - 100 µin/in-°FAverage value: 125 µm/m-°C Grade Count:27
Specific Heat Capacity 1.48 J/g-°C0.354 BTU/lb-°FAverage value: 1.48 J/g-°C Grade Count:5
Melting Point 162 - 178 °C324 - 352 °FAverage value: 167 °C Grade Count:82
Deflection Temperature at 0.46 MPa (66 psi) 95.0 - 214 °C203 - 417 °FAverage value: 136 °C Grade Count:32
Deflection Temperature at 1.8 MPa (264 psi) 40.0 - 100 °C104 - 212 °FAverage value: 76.1 °C Grade Count:100
Vicat Softening Point 60.0 - 161 °C140 - 322 °FAverage value: 124 °C Grade Count:25
Flammability, UL94 HBHBGrade Count:44
Flame Spread 41.0 - 100 mm/min1.61 - 3.94 in/minAverage value: 65.8 mm/min Grade Count:4
 
Processing PropertiesMetricEnglishComments
Processing Temperature 20.0 - 220 °C68.0 - 428 °FAverage value: 112 °C Grade Count:37
Nozzle Temperature 170 - 204 °C338 - 400 °FAverage value: 191 °C Grade Count:7
Die Temperature 180 - 200 °C356 - 392 °FAverage value: 192 °C Grade Count:26
Melt Temperature 160 - 220 °C320 - 428 °FAverage value: 188 °C Grade Count:55
Mold Temperature 40.0 - 120 °C104 - 248 °FAverage value: 71.9 °C Grade Count:40
Injection Velocity 20.0 - 50.0 mm/sec0.787 - 1.97 in/secAverage value: 35.0 mm/sec Grade Count:3
Drying Temperature 70.0 - 121 °C158 - 250 °FAverage value: 93.9 °C Grade Count:59
Moisture Content 0.0500 - 0.150 %0.0500 - 0.150 %Average value: 0.111 % Grade Count:19
Injection Pressure 3.50 - 120 MPa508 - 17400 psiAverage value: 75.7 MPa Grade Count:43
Annealing Temperature 160 °C320 °FAverage value: 160 °C Grade Count:3
Hot-Working Temperature 190 - 200 °C374 - 392 °FAverage value: 195 °C Grade Count:5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Acetal Copolymer, Unreinforced
Overview of materials for Acetal Copolymer, 10% Glass Fiber Reinforced
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced
Overview of materials for Acetal Homopolymer, Unreinforced
Overview of materials for Acetal Copolymer, Silicone Filled

O1254 / 77843

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.