MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Overview of materials for Acetal Copolymer, Impact Modified
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Impact Modified

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Impact Modified". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.07 - 1.41 g/ccAverage value: 1.35 g/cc Grade Count:116
 1.14 - 1.14 g/cc
@Temperature 205 - 205 °C
Average value: 1.14 g/cc Grade Count:2
Water Absorption 0.200 - 1.10 %Average value: 0.418 % Grade Count:32
Moisture Absorption at Equilibrium 0.200 - 0.350 %Average value: 0.237 % Grade Count:16
Water Absorption at Saturation 0.650 - 1.20 %Average value: 0.868 % Grade Count:38
Maximum Moisture Content 0.150Average value: 0.150 Grade Count:5
 0.200 - 0.200
@Temperature 100 - 100 °C
Average value: 0.200 Grade Count:2
 0.200 - 0.200
@Time 299 - 299 sec
Average value: 0.200 Grade Count:2
Linear Mold Shrinkage 0.00700 - 0.0350 cm/cmAverage value: 0.0179 cm/cm Grade Count:78
Linear Mold Shrinkage, Transverse 0.00800 - 0.0210 cm/cmAverage value: 0.0163 cm/cm Grade Count:43
Melt Flow 0.600 - 27.8 g/10 minAverage value: 7.99 g/10 min Grade Count:80
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 18.7 - 78.0Average value: 58.0 Grade Count:15
Hardness, Rockwell R 75.0 - 116Average value: 99.6 Grade Count:12
Ball Indentation Hardness 35.0 - 120 MPaAverage value: 88.6 MPa Grade Count:14
Tensile Strength, Ultimate 26.0 - 56.0 MPaAverage value: 40.6 MPa Grade Count:38
Tensile Strength, Yield 23.0 - 68.9 MPaAverage value: 44.3 MPa Grade Count:77
 22.0 - 80.0 MPa
@Temperature -40.0 - 80.0 °C
Average value: 51.0 MPa Grade Count:2
Elongation at Break 10.0 - 300 %Average value: 73.1 % Grade Count:89
Elongation at Yield 6.00 - 85.0 %Average value: 14.8 % Grade Count:64
 7.50 - 17.0 %
@Temperature -40.0 - 80.0 °C
Average value: 12.3 % Grade Count:2
Modulus of Elasticity 0.772 - 2.45 GPaAverage value: 1.70 GPa Grade Count:73
Flexural Yield Strength 24.0 - 107 MPaAverage value: 50.9 MPa Grade Count:53
Flexural Modulus 0.750 - 3.14 GPaAverage value: 1.65 GPa Grade Count:92
Poissons Ratio 0.430 - 0.440Average value: 0.433 Grade Count:3
Izod Impact, Notched 0.490 - 100 J/cmAverage value: 1.20 J/cm Grade Count:21
 0.590 - 0.907 J/cm
@Temperature -40.0 - -30.0 °C
Average value: 0.849 J/cm Grade Count:4
 1.03 - 1.03 J/cm
@Temperature -30.0 - -30.0 °C
Average value: 0.849 J/cm Grade Count:1
 1.03 - 1.03 J/cm
@Thickness 6.40 - 6.40 mm
Average value: 0.849 J/cm Grade Count:1
Izod Impact, Notched (ISO) 7.00 - 90.0 kJ/m²Average value: 17.1 kJ/m² Grade Count:19
 14.0 - 20.0 kJ/m²
@Temperature -40.0 - -30.0 °C
Average value: 17.0 kJ/m² Grade Count:2
Charpy Impact Unnotched 6.00 J/cm² - NBAverage value: 14.6 J/cm² Grade Count:56
 -4.62 J/cm² - NB
@Temperature -30.0 - -30.0 °C
Average value: 16.9 J/cm² Grade Count:44
Charpy Impact, Notched 0.500 J/cm² - NBAverage value: 1.97 J/cm² Grade Count:90
 0.504 - 1.806 J/cm²
@Temperature -30.0 - -30.0 °C
Average value: 0.935 J/cm² Grade Count:49
Coefficient of Friction 0.400 - 0.500Average value: 0.483 Grade Count:3
Penetration 5.00 - 55.0Average value: 21.0 Grade Count:7
Tensile Creep Modulus, 1 hour 700 - 1850 MPaAverage value: 1470 MPa Grade Count:24
Tensile Creep Modulus, 1000 hours 400 - 1050 MPaAverage value: 839 MPa Grade Count:24
K (wear) Factor 1.00 - 600 x 10-8 mm³/N-MAverage value: 213 x 10-8 mm³/N-M Grade Count:3
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 10000 - 1.00e+16 ohm-cmAverage value: 1.48e+15 ohm-cm Grade Count:57
Surface Resistance 260 - 1.00e+16 ohmAverage value: 2.13e+15 ohm Grade Count:57
Dielectric Constant 3.40 - 5.30Average value: 4.06 Grade Count:39
Dielectric Strength 17.7 - 86.6 kV/mmAverage value: 30.8 kV/mm Grade Count:34
Dissipation Factor 0.000600 - 0.0425Average value: 0.0116 Grade Count:35
Comparative Tracking Index 600 VAverage value: 600 V Grade Count:30
 
Thermal PropertiesOriginal ValueComments
CTE, linear 70.0 - 142 µm/m-°CAverage value: 123 µm/m-°C Grade Count:69
CTE, linear, Transverse to Flow 110 - 180 µm/m-°CAverage value: 125 µm/m-°C Grade Count:27
Specific Heat Capacity 1.48 J/g-°CAverage value: 1.48 J/g-°C Grade Count:5
Melting Point 162 - 178 °CAverage value: 167 °C Grade Count:82
Deflection Temperature at 0.46 MPa (66 psi) 95.0 - 214 °CAverage value: 136 °C Grade Count:32
Deflection Temperature at 1.8 MPa (264 psi) 40.0 - 100 °CAverage value: 76.1 °C Grade Count:100
Vicat Softening Point 60.0 - 161 °CAverage value: 124 °C Grade Count:25
Flammability, UL94 HBGrade Count:44
Flame Spread 41.0 - 100 mm/minAverage value: 65.8 mm/min Grade Count:4
 
Processing PropertiesOriginal ValueComments
Processing Temperature 20.0 - 220 °CAverage value: 112 °C Grade Count:37
Nozzle Temperature 170 - 204 °CAverage value: 191 °C Grade Count:7
Die Temperature 180 - 200 °CAverage value: 192 °C Grade Count:26
Melt Temperature 160 - 220 °CAverage value: 188 °C Grade Count:55
Mold Temperature 40.0 - 120 °CAverage value: 71.9 °C Grade Count:40
Injection Velocity 20.0 - 50.0 mm/secAverage value: 35.0 mm/sec Grade Count:3
Drying Temperature 70.0 - 121 °CAverage value: 93.9 °C Grade Count:59
Moisture Content 0.0500 - 0.150 %Average value: 0.111 % Grade Count:19
Injection Pressure 3.50 - 120 MPaAverage value: 75.7 MPa Grade Count:43
Annealing Temperature 160 °CAverage value: 160 °C Grade Count:3
Hot-Working Temperature 190 - 200 °CAverage value: 195 °C Grade Count:5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Acetal Copolymer, Unreinforced
Overview of materials for Acetal Copolymer, 10% Glass Fiber Reinforced
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced
Overview of materials for Acetal Homopolymer, Unreinforced
Overview of materials for Acetal Copolymer, Silicone Filled

O1254 / 77843

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.