MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

Aluminum 204.0-T6, Sand Cast, Precipitation Treatment 12 h at 180°C (360°F)
Categories: Metal; Nonferrous Metal; Aluminum Alloy; Aluminum Casting Alloy

Material Notes:

Composition Notes:
Composition information provided by the Aluminum Association and is not for design.

Key Words: Aluminium 204.0-T6; UNS A02040; ISO AlCu4MgTi; AA204.0-T6; Al204.0-T6
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.80 g/cc0.101 lb/in³Value for aluminum 201.0
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 125125500 kg load, 10 mm ball
Hardness, Knoop 157157Estimated from Brinell Hardness.
Hardness, Rockwell A 4848Estimated from Brinell Hardness.
Hardness, Rockwell B 7777Estimated from Brinell Hardness.
Hardness, Vickers 143143Estimated from Brinell Hardness.
Tensile Strength, Ultimate 420 MPa60900 psi
Tensile Strength, Yield 395 MPa
@Strain 0.2 %
57300 psi
@Strain 0.2 %
Elongation at Break 3.0 %3.0 %in 50 mm
Tensile Modulus 71.0 GPa10300 ksiEstimated from 206.0
Poissons Ratio 0.330.33Estimated from 206.0
Machinability 90 %90 %0-100 Scale (100=best)
Shear Modulus 26.5 GPa3840 ksiEstimated from 206.0
Shear Strength 250 MPa36300 psiCalculated
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000550 ohm-cm0.00000550 ohm-cmValue for Aluminum 201.0
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 389 J/g167 BTU/lbTypical for cast aluminum
CTE, linear  19.3 µm/m-°C
@Temperature 20.0 - 100 °C
10.7 µin/in-°F
@Temperature 68.0 - 212 °F
Value for Aluminum 201.0
 24.7 µm/m-°C
@Temperature 20.0 - 300 °C
13.7 µin/in-°F
@Temperature 68.0 - 572 °F
Value for Aluminum 201.0
Specific Heat Capacity 0.963 J/g-°C0.230 BTU/lb-°FTypical for cast aluminum
Thermal Conductivity 120 W/m-K833 BTU-in/hr-ft²-°FValue for Aluminum 201.0
Melting Point 529 - 649 °C984 - 1200 °F
Solidus 529 °C984 °F
Liquidus 649 °C1200 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 93.3 - 95.5 %93.3 - 95.5 %As remainder
Copper, Cu 4.2 - 5.0 %4.2 - 5.0 %
Iron, Fe <= 0.35 %<= 0.35 %
Magnesium, Mg 0.15 - 0.35 %0.15 - 0.35 %
Manganese, Mn <= 0.10 %<= 0.10 %
Nickel, Ni <= 0.050 %<= 0.050 %
Other, each <= 0.050 %<= 0.050 %
Other, total <= 0.15 %<= 0.15 %
Silicon, Si <= 0.20 %<= 0.20 %
Tin, Sn <= 0.050 %<= 0.050 %
Titanium, Ti 0.15 - 0.30 %0.15 - 0.30 %
Zinc, Zn <= 0.10 %<= 0.10 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum 201.0-T6 Casting Alloy
Aluminum 201.0-T7, Sand Cast
Aluminum 204.0-T6, Permanent Mold Cast, Precipitation Treatment 12 h at 180°C (360°F)
Aluminum 204.0-T6, Sand Cast, Precipitation Treatment 12 h at 140°C (285°F)
Aluminum A206.0-T7 Casting Alloy

MAC2040TS2 / 9770

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.