MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

(Viewing data as-entered. Click here to return)
Aluminum 204.0-T6, Sand Cast, Precipitation Treatment 12 h at 180°C (360°F)
Categories: Metal; Nonferrous Metal; Aluminum Alloy; Aluminum Casting Alloy

Material Notes:

Composition Notes:
Composition information provided by the Aluminum Association and is not for design.

Key Words: Aluminium 204.0-T6; UNS A02040; ISO AlCu4MgTi; AA204.0-T6; Al204.0-T6
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.80 g/ccValue for aluminum 201.0
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 125500 kg load, 10 mm ball
Hardness, Knoop 157Estimated from Brinell Hardness.
Hardness, Rockwell A 48Estimated from Brinell Hardness.
Hardness, Rockwell B 77Estimated from Brinell Hardness.
Hardness, Vickers 143Estimated from Brinell Hardness.
Tensile Strength, Ultimate 420 MPa
Tensile Strength, Yield 395 MPa
@Strain 0.2 %
Elongation at Break 3.0 %in 50 mm
Tensile Modulus 71.0 GPaEstimated from 206.0
Poissons Ratio 0.33Estimated from 206.0
Machinability 90 %0-100 Scale (100=best)
Shear Modulus 26.5 GPaEstimated from 206.0
Shear Strength 250 MPaCalculated
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000550 ohm-cmValue for Aluminum 201.0
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 389 J/gTypical for cast aluminum
CTE, linear 19.3 µm/m-°C
@Temperature 20.0 - 100 °C
Value for Aluminum 201.0
 24.7 µm/m-°C
@Temperature 20.0 - 300 °C
Value for Aluminum 201.0
Specific Heat Capacity 0.963 J/g-°CTypical for cast aluminum
Thermal Conductivity 120 W/m-KValue for Aluminum 201.0
Melting Point 529 - 649 °C
Solidus 529 °C
Liquidus 649 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 93.3 - 95.5 %As remainder
Copper, Cu 4.2 - 5.0 %
Iron, Fe <= 0.35 %
Magnesium, Mg 0.15 - 0.35 %
Manganese, Mn <= 0.10 %
Nickel, Ni <= 0.050 %
Other, each <= 0.050 %
Other, total <= 0.15 %
Silicon, Si <= 0.20 %
Tin, Sn <= 0.050 %
Titanium, Ti 0.15 - 0.30 %
Zinc, Zn <= 0.10 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aluminum 201.0-T6 Casting Alloy
Aluminum 201.0-T7, Sand Cast
Aluminum 204.0-T6, Permanent Mold Cast, Precipitation Treatment 12 h at 180°C (360°F)
Aluminum 204.0-T6, Sand Cast, Precipitation Treatment 12 h at 140°C (285°F)
Aluminum A206.0-T7 Casting Alloy

MAC2040TS2 / 9770

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.