MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Mitsubishi Chemical Advanced Materials TIVAR® 1000 ASTL UHMW-PE + specific additives (ISO Data)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); UHMW PE (Ultra High Molecular Weight PE)

Material Notes: TIVAR 1000 ASTL, based on a UHMW-PE grade with extremely high molecular weight, has been specifically developed for tough anti-abrasion applications. TIVAR 1000 ASTL shows a higher wear and abrasion resistance and a lower surface resistivity than TIVAR 1000 antistatic. The additives used also render this material static dissipative and highly UV-resistant.

  • Very good wear and abrasion resistance
  • High impact strength, even at low temperatures (particularly UHMW-PE)
  • Excellent chemical resistance
  • Low coefficient of friction
  • Excellent release properties
  • Very low water absorption
  • Moderate mechanical strength, stiffness and creep resistance
  • Very good electrical insulating and dielectric properties (except static dissipative grades)
  • Excellent machinability
  • Physiologically inert (several grades are suitable for food contact)
  • Good resistance to high energy radiation (gamma- and X-rays)
  • Not self-extinguishing
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 0.950 g/cc0.0343 lb/in³ISO 1183-1
Water Absorption <= 0.10 %<= 0.10 %96 hr; ISO 62
Moisture Absorption at Equilibrium <= 0.10 %<= 0.10 %50% RH
Water Absorption at Saturation <= 0.10 %<= 0.10 %ISO 62
Outgassing - Total Mass Loss 0.14 %0.14 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6161
Ball Indentation Hardness 34.0 MPa4930 psiISO 2039-1
Tensile Strength 21.0 MPa3050 psiat Yield; ISO 527-1/-2
Elongation at Break >= 50 %>= 50 %ISO 527-1/-2
Elongation at Yield 15 %15 %ISO 527-1/-2
Tensile Modulus 0.800 GPa116 ksiISO 527-1/-2
Flexural Strength 19.0 MPa2760 psi
Compressive Strength  7.00 MPa
@Strain 1 %
1020 psi
@Strain 1 %
ISO 604
 11.5 MPa
@Strain 2 %
1670 psi
@Strain 2 %
ISO 604
 18.0 MPa
@Strain 5.0 %
2610 psi
@Strain 5.0 %
ISO 604
K Factor (ISO) 6.0 µm/km6.0 µm/km
Charpy Impact Unnotched NBNBISO 179-1/1eU
Charpy Impact, Notched 9.00 J/cm²42.8 ft-lb/in²Partial Break; ISO 179-1/1eA
Coefficient of Friction, Dynamic 0.15 - 0.300.15 - 0.30
Sand Slurry 8585
Limiting Pressure Velocity 0.0500 MPa-m/sec1430 psi-ft/minat 1 m/s unlubricated
 0.0800 MPa-m/sec2280 psi-ft/minat 0.1 m/s unlubricated
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square <= 1.0e+6 ohm<= 1.0e+6 ohmIEC 60093
 
Thermal PropertiesMetricEnglishComments
CTE, linear 200 µm/m-°C
@Temperature 23.0 - 100 °C
111 µin/in-°F
@Temperature 73.4 - 212 °F
Thermal Conductivity 0.400 W/m-K2.78 BTU-in/hr-ft²-°F
Melting Point 135 °C275 °FDSC, 10°C/min.; ISO 11357-1/-3
Maximum Service Temperature, Air 80.0 °C176 °FContinuous
Deflection Temperature at 1.8 MPa (264 psi) 42.0 °C108 °FISO 75-1/-2
Flammability, UL94 HBHB
Oxygen Index <= 20 %<= 20 %ISO 4589-1/-2
 
Compliance PropertiesMetricEnglishComments
3A-Dairy NoNo
European Food 1935/2004 YesYes
FDA NoNo
USP Class VI NoNo
 
Chemical Resistance PropertiesMetricEnglishComments
Acids, Strong (pH 1-3) AcceptableAcceptable
Acids, Weak AcceptableAcceptable
Alcohols AcceptableAcceptable
Alkalies, Strong (pH 11-14) AcceptableAcceptable
Alkalies, Weak AcceptableAcceptable
Chlorinated Solvents AcceptableAcceptable
Conductive / Static Dissipative YesYes
Continuous Sunlight LimitedLimited
Hot Water / Steam UnacceptableUnacceptable
Hydrocarbons - Aliphatic AcceptableAcceptable
Hydrocarbons - Aromatic LimitedLimited
Inorganic Salt Solutions AcceptableAcceptable
Ketones, Esters AcceptableAcceptable

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials TIVAR® 1000 UHMW-PE, (Natural & Colors except Black) (ASTM Product Data Sheet)
Mitsubishi Chemical Advanced Materials TIVAR® 1000 EC Electrically Conductive UHMW-PE (ASTM Product Data Sheet)
Mitsubishi Chemical Advanced Materials TIVAR® CleanStat™ Electro Static Dissipative UHMW-PE (ASTM Product Data Sheet)
GEHR Plastics PE-UHMW Polyethylene, Ultra High Molecular Weight
Mitsubishi Chemical Advanced Materials TIVAR® MD UHMW-PE, FDA Metal Detectable (ASTM Product Data Sheet)

P1SMU940 / 130710

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.