MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Total 7835XM Polypropylene, Blow Molding Grade  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Blow Molding Grade

Material Notes: Random copolymer injection stretch blow molding grade

Clarified - FINA 7835XM offers the ultimate in clarity and gloss.

Impact Strength - FINA 7835XM offers an excellent balance of impact strength and stiffness.

High Purity - FINA 7835XM features minimum taste and odor, an optimum thermal stability for superior color and processability.

FDA - FINA 7835XM complies with all applicable FDA regulations and may be used under those provisions for food contact and packaging.

Recommended Applications - FINA 7835XM is optimized for injection stretch blow molding of containers for drug, cosmetic and toiletry applications requiring exceptional clarity.

Processing - FINA 7835XM resin processes on conventional blow molding equipment with typical melt temperatures of 390-450°F (199-232°C)

Data provided by the manufacturer, Total Petrochemicals.

Total Petrochemicals includes former Fina and Atofina plastics product lines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Water Vapor Permeability 9.40 g mil/ (m2 day)
@Temperature 37.8 °C
0.606 g mil/ (100 in2 day)
@Temperature 100 °F
90% RH; ASTM E96
Density 0.900 g/cc0.0325 lb/in³ASTM D1505
Oxygen Transmission 95.0 cc-mm/m²-24hr-atm
@Temperature 23.0 °C
241 cc-mil/100 in²-24hr-atm
@Temperature 73.4 °F
cc-mm/m²-24hr-atm; ASTM D1434
Linear Mold Shrinkage 0.010 - 0.025 cm/cm0.010 - 0.025 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 28.0 MPa4060 psiASTM D638
Elongation at Break 10 %10 %ASTM D638
Modulus of Elasticity 1.10 GPa160 ksiASTM D638
Flexural Modulus 0.900 GPa131 ksiASTM D790
Izod Impact, Notched 0.690 J/cm1.29 ft-lb/inASTM D256A
 
Thermal PropertiesMetricEnglishComments
Melting Point 143 °C289 °FDSC
Deflection Temperature at 0.46 MPa (66 psi) 82.0 °C180 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Melt Temperature 200 - 232 °C392 - 450 °Fblow molding

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Flint Hills P5L2K-055 Polypropylene Random Copolymer
Braskem H 604 Blow Molding Polypropylene
Total PPH 3230 Polypropylene, Blow Molding Grade
Total 7426MZ Polypropylene, Blow Molding Grade
Phillips Sumika Marlex® RGC-020 Polypropylene Random Copolymer, Clarified

PFINA3 / 38433

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.