MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Flint Hills P5L2K-055 Polypropylene Random Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer; Polypropylene, Blow Molding Grade; Polypropylene, Extrusion Grade

Material Notes: Features: Excellent clarity. Product does not contain animal derived components. Phthalate-free.

Applications: Injection molding: extrusion blow molding, injection blow molding, stretch blow molding, clear containers and hot fill applications.

Information Provided by Flint Hills Resources

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ASTM D1505
Melt Flow 1.9 g/10 min1.9 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 9393ASTM D785
Tensile Strength, Yield 36.0 MPa5220 psiASTM D638
Elongation at Break 11 %11 %ASTM D638
Flexural Modulus, 1% Secant 1270 MPa184000 psiASTM D790
Izod Impact, Notched 0.500 J/cm
@Temperature 23.0 °C
0.937 ft-lb/in
@Temperature 73.4 °F
ASTM D256
Gardner Impact 1.00 J
@Temperature -30.0 °C
0.738 ft-lb
@Temperature -22.0 °F
ASTM D5420
Tangent Modulus 1300 MPa189000 psiASTM D790
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 89.0 °C192 °FASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Flint Hills AP5325-HS Impact Copolymer Polypropylene
Flint Hills P5M6K-080 Polypropylene Random Copolymer
Total PPH 3720WZ Polypropylene, Injection Molding Grade
Flint Hills 23S2A Polypropylene Random Copolymer
Flint Hills P5M2Z-012 Polypropylene Random Copolymer

PFLINT025 / 104579

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.