MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Eurotec® Tecotek® PC30 NL VB03 PC, unfilled, UV stabilized, high impact, natural
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Impact Modified; Polycarbonate, UV Stabilized

Material Notes:

Information provided by Eurotec®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.21 g/cc0.0437 lb/in³ISO 1183
Moisture Absorption 0.200 %
@Temperature 23.0 °C
0.200 %
@Temperature 73.4 °F
50% RH; ISO 960
Linear Mold Shrinkage, Flow 0.0080 cm/cm0.0080 in/inEurotec
Linear Mold Shrinkage, Transverse 0.0080 cm/cm0.0080 in/inEurotec
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 55.0 MPa7980 psiISO 527
Elongation at Break >= 50 %>= 50 %ISO 527
Tensile Modulus 2.25 GPa326 ksiISO 527
Izod Impact, Notched (ISO)  25.0 kJ/m²
@Temperature -30.0 °C
11.9 ft-lb/in²
@Temperature -22.0 °F
ISO 180/1A
 55.0 kJ/m²
@Temperature 23.0 °C
26.2 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1A
Izod Impact, Unnotched (ISO)  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 180/1U
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 180/1U
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+15 ohm1.00e+15 ohmIEC 60093
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 120 °C248 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C203 °FISO 75
Vicat Softening Point 125 °C
@Load 5.10 kg
257 °F
@Load 11.2 lb
ISO 306
Flammability, UL94  HB
@Thickness 0.750 mm
HB
@Thickness 0.0295 in
 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
 
Processing PropertiesMetricEnglishComments
Processing Temperature 260 - 280 °C500 - 536 °F
Feed Temperature 60.0 - 80.0 °C140 - 176 °FThroat
Mold Temperature 80.0 - 100 °C176 - 212 °F
Drying Temperature 110 °C230 °F
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hour
Moisture Content <= 0.10 %<= 0.10 %ISO 960
Hold Pressure 50.0 - 100 MPa7250 - 14500 psi
 
Descriptive Properties
Back PressureLow
Injection SpeedMedium - Fast

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mitsubishi Xantar® G4F 23 UR Polycarbonate-20% Glass Reinforced
Lehvoss LUVOCOM® 50/TF/15/BK Polycarbonate with PTFE
LG Chemical LUPOY SC2202 PC+GF20%, High Impact
Covestro Apec® HT KU 1-9331 High-Heat Polycarbonate
Covestro Makrolon® 8325 Polycarbonate

PEUROS155 / 147145

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.