MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Silver-Palladium Alloy, 59Ag-25Pd
Categories: Metal; Nonferrous Metal; Precious Metal; Silver Alloy

Material Notes: Composition reported in reference does not add to 100%.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 10.5 g/cc0.379 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 235235
Tensile Strength, Ultimate 751 MPa109000 psi
Tensile Strength, Yield 660 MPa
@Strain 0.2 %
95700 psi
@Strain 0.2 %
Elongation at Break 9.0 %9.0 %
 
Thermal PropertiesMetricEnglishComments
Melting Point 900 - 980 °C1650 - 1800 °F
Solidus 900 °C1650 °F
Liquidus 980 °C1800 °F
 
Component Elements PropertiesMetricEnglishComments
Palladium, Pd 25 %25 %
Silver, Ag 59 %59 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Zinc Alloy 7; AG40B; Zn-4Al-0.015Mg; Zamak7
Zinc AC41A Alloy (Zamak 5), As Cast
AISI 81B45 Steel
90Ag-10Pd Alloy, Annealed
50Ag-50Pd Alloy, Annealed

MPAgS95 / 100389

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.