MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Trinseo CALIBRE™ MEGARAD™ 2081-22 Polycarbonate Resin
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Gamma Radiation Resistant

Material Notes: CALIBRE™ MEGARAD 2081-22 Polycarbonate resin is a high-flow resin designed for injection molded medical parts. It is stabilized to reduce color shift associated with exposed to high energy radiation (gamma or electron beam). It is available in light purple transparent color designation FC300006.

Main Characteristics:

  • Stabilized for higher energy radiation
  • Tested under ISO 10993
  • Transparent
  • Contains mold release
Applications:
  • Medical applications

Information provided by Trinseo.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ASTM D792
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm0.0050 - 0.0070 in/inASTM D955
Melt Flow 22 g/10 min
@Load 1.20 kg,
Temperature 300 °C
22 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 46.9 MPa6800 psi50 mm/min; ASTM D638
Tensile Strength, Yield 64.1 MPa9300 psi50 mm/min; ASTM D638
Elongation at Break 180 %180 %50 mm/min; ASTM D638
Izod Impact, Notched 7.50 J/cm14.1 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 123 °C253 °FUnannealed; ASTM D648
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 85 %85 %ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Trinseo CALIBRE™ MEGARAD™ 2081-15 Polycarbonate Resin
Overview of materials for Polycarbonate, Optical Grade
Trinseo CALIBRE™ 2060 10 Polycarbonate, Sterilization Grade
Trinseo CALIBRE™ 2061-15 Polycarbonate Resin
Trinseo CALIBRE™ 5051 15 Polycarbonate, 5% Glass Reinforced

PDWST048 / 142257

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.