Physical Properties | Metric | English | Comments |
---|
Density | 0.00800 - 1.39 g/cc | 0.000289 - 0.0504 lb/in³ |
| 0.159559 - 0.161321 g/cc @Temperature 121 - 177 °C | 0.00576444 - 0.00582811 lb/in³ @Temperature 250 - 350 °F |
Water Absorption | 0.0100 - 72.0 % | 0.0100 - 72.0 % |
Moisture Absorption at Equilibrium | 2.00 % | 2.00 % |
Water Absorption at Saturation | 0.300 - 20.0 % | 0.300 - 20.0 % |
Viscosity | 23.0 - 27500 cP | 23.0 - 27500 cP |
| 310 - 17000 cP @Temperature 15.6 - 48.9 °C | 310 - 17000 cP @Temperature 60.0 - 120 °F |
Thickness | 27.9 - 12700 microns | 1.10 - 500 mil |
Linear Mold Shrinkage | 0.000800 - 0.0110 cm/cm | 0.000800 - 0.0110 in/in |
Outgassing - Total Mass Loss | 0.300 - 1.73 % @Temperature 125 - 125 °C | 0.300 - 1.73 % @Temperature 257 - 257 °F |
| 0.300 - 1.73 % @Time 86400 - 86400 sec | 0.300 - 1.73 % @Time 24.0 - 24.0 hour |
|
Mechanical Properties | Metric | English | Comments |
---|
Hardness, Shore A | 3.00 - 60.0 | 3.00 - 60.0 |
Hardness, Shore D | 3.50 - 95.0 | 3.50 - 95.0 |
Hardness, Shore O | 2.00 - 65.0 | 2.00 - 65.0 |
Hardness, Shore OO | 10.0 - 45.0 | 10.0 - 45.0 |
Tensile Strength, Ultimate | 0.0207 - 1900 MPa | 3.00 - 276000 psi |
| 0.799792 - 1.24795 MPa @Temperature 121 - 177 °C | 116.000 - 181.000 psi @Temperature 250 - 350 °F |
Tensile Strength, Yield | 0.0814 - 103 MPa | 11.8 - 15000 psi |
Film Elongation at Break, MD | 78.0 % | 78.0 % |
| 74.0 - 74.0 % @Temperature 66.0 - 66.0 °C | 74.0 - 74.0 % @Temperature 151 - 151 °F |
| 74.0 - 74.0 % @Time 346000 - 346000 sec | 74.0 - 74.0 % @Time 96.0 - 96.0 hour |
Film Elongation at Break, TD | 32.0 % | 32.0 % |
| 66.0 - 66.0 % @Temperature 66.0 - 66.0 °C | 66.0 - 66.0 % @Temperature 151 - 151 °F |
| 66.0 - 66.0 % @Time 346000 - 346000 sec | 66.0 - 66.0 % @Time 96.0 - 96.0 hour |
Elongation at Break | 3.20 - 760 % | 3.20 - 760 % |
Elongation at Yield | 301 - 409 % | 301 - 409 % |
Modulus of Elasticity | 0.000138 - 3.45 GPa | 0.0200 - 500 ksi |
| 0.000287511 - 0.0145893 GPa @Temperature 71.1 - 71.1 °C | 0.0417007 - 2.11603 ksi @Temperature 160 - 160 °F |
Flexural Yield Strength | 0.207 - 56.5 MPa | 30.0 - 8190 psi |
Flexural Modulus | 0.00407 - 1.93 GPa | 0.590 - 280 ksi |
Compressive Yield Strength | 0.00172 - 48.0 MPa | 0.250 - 6960 psi |
| 0.0689476 - 44.1195 MPa @Temperature -53.9 - 177 °C | 10.0000 - 6399.01 psi @Temperature -65.0 - 350 °F |
| 0.124106 - 0.124106 MPa @Temperature 65.6 - 65.6 °C | 18.0000 - 18.0000 psi @Temperature 150 - 150 °F |
| 0.124106 - 0.124106 MPa @Strain 25.0 - 25.0 % | 18.0000 - 18.0000 psi @Strain 25.0 - 25.0 % |
Compressive Modulus | 0.0000276 - 1.28 GPa | 0.00400 - 186 ksi |
| 0.00169611 - 0.556862 GPa @Temperature -53.9 - 177 °C | 0.246004 - 80.7673 ksi @Temperature -65.0 - 350 °F |
Resilience | 29.0 - 52.0 | 29.0 - 52.0 |
Rebound | 19.0 - 31.0 % | 19.0 - 31.0 % |
Poissons Ratio | 0.300 - 0.750 | 0.300 - 0.750 |
Shear Modulus | 0.00152 - 8.01 GPa | 0.220 - 1160 ksi |
Shear Strength | 0.0896 - 30.2 MPa | 13.0 - 4390 psi |
| 1.08937 - 1.40653 MPa @Temperature 121 - 177 °C | 158.000 - 204.000 psi @Temperature 250 - 350 °F |
Izod Impact, Unnotched | 0.347 - 0.972 J/cm | 0.650 - 1.82 ft-lb/in |
Charpy Impact Unnotched | 0.378 J/cm² - NB | 1.80 ft-lb/in² - NB |
Charpy Impact, Notched | 0.380 - 1.40 J/cm² | 1.81 - 6.66 ft-lb/in² |
Coefficient of Friction | 0.400 - 1.40 | 0.400 - 1.40 |
Tear Strength Test | 30.0 - 137 | 30.0 - 137 |
Tear Strength | 0.140 - 10.5 kN/m | 0.800 - 60.0 pli |
Peel Strength | 0.438 - 0.892 kN/m | 2.50 - 5.09 pli |
Compression Set | 0.000 - 87.3 % | 0.000 - 87.3 % |
Seal Strength | 9.40 g/25 mm | 9.40 g/in |
| 10.6 - 10.6 g/25 mm @Temperature 66.0 - 66.0 °C | 10.6 - 10.6 g/in @Temperature 151 - 151 °F |
| 10.6 - 10.6 g/25 mm @Time 346000 - 346000 sec | 10.6 - 10.6 g/in @Time 96.0 - 96.0 hour |
Film Tensile Strength at Break, MD | 207 MPa | 30000 psi |
|
Electrical Properties | Metric | English | Comments |
---|
Electrical Resistivity | 3.00e+10 - 1.00e+15 ohm-cm | 3.00e+10 - 1.00e+15 ohm-cm |
Surface Resistance | 0.100 - 2.00e+14 ohm | 0.100 - 2.00e+14 ohm |
| 0.00700 - 0.0170 ohm @Temperature 35.0 - 121 °C | 0.00700 - 0.0170 ohm @Temperature 95.0 - 250 °F |
| 0.00700 - 0.0170 ohm @Time 605000 - 7.88e+6 sec | 0.00700 - 0.0170 ohm @Time 168 - 2190 hour |
Shielding Effectiveness | 62.0 - 110 dB | 62.0 - 110 dB |
Dielectric Constant | 1.04 - 1.75 | 1.04 - 1.75 |
Dielectric Strength | 1.65 - 18.0 kV/mm | 42.0 - 457 kV/in |
Dissipation Factor | 0.00187 - 0.0500 | 0.00187 - 0.0500 |
|
Thermal Properties | Metric | English | Comments |
---|
CTE, linear | 7.20 - 630 µm/m-°C | 4.00 - 350 µin/in-°F |
| 61.2 - 72.0 µm/m-°C @Temperature 23.9 - 121 °C | 34.0 - 40.0 µin/in-°F @Temperature 75.0 - 250 °F |
Specific Heat Capacity | 0.983 - 1.57 J/g-°C | 0.235 - 0.376 BTU/lb-°F |
Thermal Conductivity | 0.00591 - 0.830 W/m-K | 0.0410 - 5.76 BTU-in/hr-ft²-°F |
Insulation R Value | 1.57 - 23.5 | 1.57 - 23.5 |
Maximum Service Temperature, Air | 66.0 - 177 °C | 151 - 350 °F |
Deflection Temperature at 0.46 MPa (66 psi) | 47.0 - 100 °C | 117 - 212 °F |
Minimum Service Temperature, Air | -196 - 0.000 °C | -320 - 32.0 °F |
Brittleness Temperature | -51.0 - -12.0 °C | -59.8 - 10.4 °F |
Glass Transition Temp, Tg | 42.8 - 149 °C | 109 - 300 °F |
Flammability, UL94 | HB - 5VB | HB - 5VB |
Flame Spread Index | 10.0 - 25.0 | 10.0 - 25.0 |
Flash Point | 93.0 - 213 °C | 199 - 415 °F |
|
Optical Properties | Metric | English | Comments |
---|
Transmission, Visible | 90.0 % | 90.0 % |
|
Processing Properties | Metric | English | Comments |
---|
Processing Temperature | 21.1 - 60.0 °C | 70.0 - 140 °F |
Mold Temperature | 21.1 - 76.0 °C | 70.0 - 169 °F |
Cure Time | 0.417 - 4320 min | 0.00694 - 72.0 hour |
| 15.0 - 480 min @Temperature 43.3 - 121 °C | 0.250 - 8.00 hour @Temperature 110 - 250 °F |
Pot Life | 0.167 - 6.00 min | 0.167 - 6.00 min |
Some of the values displayed above may have been converted from their original units and/or rounded in order to
display the information in a consistent format. Users requiring more precise data for scientific or engineering
calculations can click on the property value to see the original value as well as raw conversions to equivalent units.
We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding
error. We also ask that you refer to MatWeb's
terms of use regarding this information.
Click here to view
all the property values for this datasheet as they were originally entered into MatWeb.