MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Xenon, Xe
Categories: Fluid; Pure Element

Material Notes: Physical Form: Colorless Gas

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.005366 g/cc0.0001939 lb/in³Gas
 
Chemical PropertiesMetricEnglishComments
Atomic Mass 131.29131.291995
Atomic Number 5454
X-ray Absorption Edge 0.35849 Å0.35849 ÅK
 2.27449 Å2.27449 ÅLI
 2.43058 Å2.43058 ÅLII
 2.5933 Å2.5933 ÅLIII
Critical Pressure 58.4100 bar43811.1 torr
Critical Temperature 16.62 °C61.92 °F
Critical Molar Volume 118 cm³/mol7.20 in³/mol
Electronegativity 2.62.6Pauling
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 17.29 J/g7.438 BTU/lb
Heat of Vaporization 95.74 J/g41.19 BTU/lbAt Boiling Point
Specific Heat Capacity 0.1584 J/g-°C0.03787 BTU/lb-°FGas
Thermal Conductivity  0.00200 W/m-K
@Pressure 0.000 MPa,
Temperature -173 °C
0.0139 BTU-in/hr-ft²-°F
@Pressure 0.000 psi,
Temperature -280 °F
gas; low pressure limiting value
 0.00360 W/m-K
@Pressure 0.000 MPa,
Temperature -73.1 °C
0.0250 BTU-in/hr-ft²-°F
@Pressure 0.000 psi,
Temperature -99.7 °F
gas; low pressure limiting value
 0.00550 W/m-K
@Pressure 0.000 MPa,
Temperature 26.9 °C
0.0382 BTU-in/hr-ft²-°F
@Pressure 0.000 psi,
Temperature 80.3 °F
gas; low pressure limiting value
 0.00730 W/m-K
@Pressure 0.000 MPa,
Temperature 127 °C
0.0507 BTU-in/hr-ft²-°F
@Pressure 0.000 psi,
Temperature 260 °F
gas; low pressure limiting value
 0.00890 W/m-K
@Pressure 0.000 MPa,
Temperature 227 °C
0.0618 BTU-in/hr-ft²-°F
@Pressure 0.000 psi,
Temperature 440 °F
gas; low pressure limiting value
 0.0104 W/m-K
@Pressure 0.000 MPa,
Temperature 327 °C
0.0722 BTU-in/hr-ft²-°F
@Pressure 0.000 psi,
Temperature 620 °F
gas; low pressure limiting value
Melting Point -111.79 °C-169.22 °F
Boiling Point -108.12 °C-162.62 °F
Heat of Formation 0.000 kJ/mol0.000 kJ/molGas
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.3918
@Temperature -112 °C,
Wavelength 546 nm
1.3918
@Temperature -170 °F,
Wavelength 546 nm
 
Component Elements PropertiesMetricEnglishComments
Xenon, Xe 100 %100 %
 
Descriptive Properties
AppearanceColorless Gas
CAS Number7440-63-3
SolubilitySlightly Soluble in H2O

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
EMS-Grivory Grilamid® XE 3817 black 9992 PA12
Hafnium, Hf; Plate
Hafnium, Hf; Rod
Hafnium, Hf; Strip
Hydrogen Fluoride, HF

AMEXe / 128

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.