MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Baygal® 90 IK 20 Polyurethane  (discontinued **)
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Liquid, Quartz Filled

Material Notes: Uses: Suitable for the production of parts: for example: insulators, bushing insulators, components of switchgear cabinets.

Information provided by Bayer.

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.80 g/cc0.0650 lb/in³
Water Absorption at Saturation 0.050 %0.050 %
 0.050 %0.050 %
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 88.0 MPa12800 psi
Elongation at Break 1.3 %1.3 %
Tensile Modulus 9.10 GPa1320 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cm
Surface Resistance >= 1.00e+15 ohm>= 1.00e+15 ohm
Dielectric Constant  4.3
@Frequency 1e+6 Hz
4.3
@Frequency 1e+6 Hz
 4.5
@Frequency 100 Hz
4.5
@Frequency 100 Hz
Dielectric Strength 32.0 kV/mm813 kV/in
Dissipation Factor  0.013
@Frequency 100 Hz
0.013
@Frequency 100 Hz
 0.015
@Frequency 1e+6 Hz
0.015
@Frequency 1e+6 Hz
Comparative Tracking Index 600 V600 V
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 34.0 µm/m-°C
@Temperature 20.0 °C
18.9 µin/in-°F
@Temperature 68.0 °F
CTE, linear, Transverse to Flow 34.0 µm/m-°C
@Temperature 20.0 °C
18.9 µin/in-°F
@Temperature 68.0 °F
Glass Transition Temp, Tg 140 °C284 °F
Oxygen Index 35 %35 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Baydur® 110 FR Polyurethane
Covestro Baygal® 90 IK 51 Polyurethane
Covestro Baygal® 90 IK 69 Polyurethane
Dow VORANOL™ 4240 Polyether Polyol
Dow VORANOL™ 4701 Polyether Polyol

PBA070 / 26682

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.