MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Covestro Baygal® 90 IK 20 Polyurethane  (discontinued **)
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Liquid, Quartz Filled

Material Notes: Uses: Suitable for the production of parts: for example: insulators, bushing insulators, components of switchgear cabinets.

Information provided by Bayer.

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.80 g/cc
Water Absorption at Saturation 0.050 %
 0.050 %
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 88.0 MPa
Elongation at Break 1.3 %
Tensile Modulus 9.10 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity >= 1.00e+15 ohm-cm
Surface Resistance >= 1.00e+15 ohm
Dielectric Constant 4.3
@Frequency 1e+6 Hz
 4.5
@Frequency 100 Hz
Dielectric Strength 32.0 kV/mm
Dissipation Factor 0.013
@Frequency 100 Hz
 0.015
@Frequency 1e+6 Hz
Comparative Tracking Index 600 V
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 34.0 µm/m-°C
@Temperature 20.0 °C
CTE, linear, Transverse to Flow 34.0 µm/m-°C
@Temperature 20.0 °C
Glass Transition Temp, Tg 140 °C
Oxygen Index 35 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Baydur® 110 FR Polyurethane
Covestro Baygal® 90 IK 51 Polyurethane
Covestro Baygal® 90 IK 69 Polyurethane
Dow VORANOL™ 4240 Polyether Polyol
Dow VORANOL™ 4701 Polyether Polyol

PBA070 / 26682

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.