MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Nylon 6, Mineral Reinforced, Impact Grade
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Mineral Reinforced, Impact Grade

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Mineral Reinforced, Impact Grade". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.17 - 1.55 g/cc0.0423 - 0.0560 lb/in³Average value: 1.34 g/cc Grade Count:14
 1.109 - 1.109 g/cc
@Temperature >=220 °C
0.04007 - 0.04007 lb/in³
@Temperature >=428 °F
Average value: 1.11 g/cc Grade Count:1
Linear Mold Shrinkage 0.00200 - 0.0140 cm/cm0.00200 - 0.0140 in/inAverage value: 0.00936 cm/cm Grade Count:9
Linear Mold Shrinkage, Transverse 0.00750 - 0.0130 cm/cm0.00750 - 0.0130 in/inAverage value: 0.0102 cm/cm Grade Count:3
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 30.0 - 100 MPa4350 - 14500 psiAverage value: 64.9 MPa Grade Count:9
Tensile Strength, Yield 53.0 - 76.0 MPa7690 - 11000 psiAverage value: 67.1 MPa Grade Count:5
Elongation at Break 2.00 - 45.0 %2.00 - 45.0 %Average value: 15.7 % Grade Count:13
Modulus of Elasticity 1.40 - 5.17 GPa203 - 750 ksiAverage value: 3.35 GPa Grade Count:5
Flexural Yield Strength 59.0 - 120 MPa8560 - 17400 psiAverage value: 94.6 MPa Grade Count:13
Flexural Modulus 1.60 - 8.80 GPa232 - 1280 ksiAverage value: 4.06 GPa Grade Count:13
Izod Impact, Notched 0.480 - 1.49 J/cm0.899 - 2.79 ft-lb/inAverage value: 0.907 J/cm Grade Count:5
Izod Impact, Unnotched 6.41 J/cm - NB12.0 ft-lb/in - NBAverage value: 6.41 J/cm Grade Count:3
Charpy Impact Unnotched 2.00 - 100 J/cm²9.52 - 476 ft-lb/in²Average value: 23.6 J/cm² Grade Count:5
 1.50 - 1.50 J/cm²
@Temperature -20.0 - -20.0 °C
7.14 - 7.14 ft-lb/in²
@Temperature -4.00 - -4.00 °F
Average value: 1.50 J/cm² Grade Count:1
Charpy Impact, Notched 0.500 - 1.20 J/cm²2.38 - 5.71 ft-lb/in²Average value: 0.750 J/cm² Grade Count:6
 0.390 - 0.400 J/cm²
@Temperature -30.0 - -20.0 °C
1.86 - 1.90 ft-lb/in²
@Temperature -22.0 - -4.00 °F
Average value: 0.395 J/cm² Grade Count:2
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+15 - 1.00e+17 ohm-cm1.00e+15 - 1.00e+17 ohm-cmAverage value: 2.57e+16 ohm-cm Grade Count:4
 
Thermal PropertiesMetricEnglishComments
Melting Point 205 - 259 °C401 - 498 °FAverage value: 223 °C Grade Count:9
Deflection Temperature at 0.46 MPa (66 psi) 170 - 191 °C338 - 376 °FAverage value: 179 °C Grade Count:3
Deflection Temperature at 1.8 MPa (264 psi) 58.0 - 220 °C136 - 428 °FAverage value: 116 °C Grade Count:13
Flammability, UL94 HB - V-0HB - V-0Grade Count:4
 
Processing PropertiesMetricEnglishComments
Processing Temperature 221 - 275 °C430 - 527 °FAverage value: 253 °C Grade Count:3
Melt Temperature 200 - 305 °C392 - 581 °FAverage value: 258 °C Grade Count:9
Mold Temperature 40.0 - 120 °C104 - 248 °FAverage value: 73.8 °C Grade Count:10
Drying Temperature 80.0 - 130 °C176 - 266 °FAverage value: 95.0 °C Grade Count:8
Moisture Content 0.150 - 0.200 %0.150 - 0.200 %Average value: 0.183 % Grade Count:3
Injection Pressure 34.0 - 138 MPa4930 - 20000 psiAverage value: 86.4 MPa Grade Count:5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Nylon 6, 30% Mineral Filled
Overview of materials for Nylon 6, Glass/Mineral Reinforced
Overview of materials for Nylon 6, 20% Mineral Filled
Overview of materials for Nylon 66/6, Mineral Reinforced
Overview of materials for Nylon 6, 40% Mineral Filled

O2427 / 77985

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.