MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Heavy Water, Deuterium Oxide, D2O
Categories: Fluid

Key Words: Deuterated Water, D2O
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density  1.0635 g/cc
@Temperature 100 °C
0.038421 lb/in³
@Temperature 212 °F
at 1 bar
 1.0712 g/cc
@Temperature 90.0 °C
0.038700 lb/in³
@Temperature 194 °F
at 1 bar
 1.0783 g/cc
@Temperature 80.0 °C
0.038956 lb/in³
@Temperature 176 °F
at 1 bar
 1.0847 g/cc
@Temperature 70.0 °C
0.039187 lb/in³
@Temperature 158 °F
at 1 bar
 1.0905 g/cc
@Temperature 60.0 °C
0.039397 lb/in³
@Temperature 140 °F
at 1 bar
 1.0957 g/cc
@Temperature 50.0 °C
0.039585 lb/in³
@Temperature 122 °F
at 1 bar
 1.1001 g/cc
@Temperature 40.0 °C
0.039744 lb/in³
@Temperature 104 °F
at 1 bar
 1.1034 g/cc
@Temperature 30.0 °C
0.039863 lb/in³
@Temperature 86.0 °F
at 1 bar
 1.1044 g/cc
@Temperature 25.0 °C
0.039899 lb/in³
@Temperature 77.0 °F
at 1 bar
 1.105 g/cc
@Temperature 20.0 °C
0.03992 lb/in³
@Temperature 68.0 °F
at 1 bar
 1.1053 g/cc
@Temperature 3.80 °C
0.039931 lb/in³
@Temperature 38.8 °F
at 1 bar
 1.1055 g/cc
@Temperature 5.00 °C
0.039939 lb/in³
@Temperature 41.0 °F
at 1 bar
 1.1056 g/cc
@Temperature 15.0 °C
0.039942 lb/in³
@Temperature 59.0 °F
at 1 bar
 1.1057 g/cc
@Temperature 10.0 °C
0.039946 lb/in³
@Temperature 50.0 °F
at 1 bar
Viscosity 1.2467 cP
@Temperature 20.0 °C
1.2467 cP
@Temperature 68.0 °F
Dynamic Viscosity
Molecular Weight 20.027 g/mol20.027 g/mol
Vapor Pressure 0.02734 bar
@Temperature 20.0 °C
20.51 torr
@Temperature 68.0 °F
Surface Tension 71.87 dynes/cm
@Temperature 20.0 °C
71.87 dynes/cm
@Temperature 68.0 °F
 
Chemical PropertiesMetricEnglishComments
Critical Pressure 216.71 bar162550 torr
Critical Temperature 370.7 °C699.3 °F
Critical Density 0.356 g/cc0.0129 lb/in³
Critical Molar Volume 56.0 cm³/mol3.42 in³/mol
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 78.06
@Temperature 20.0 °C
78.06
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
Heat of Vaporization 2064 J/g887.8 BTU/lb
CTE, linear 57.0 µm/m-°C
@Temperature 20.0 °C
31.7 µin/in-°F
@Temperature 68.0 °F
converted to linear from cubic CTE
Specific Heat Capacity 4.228 J/g-°C
@Temperature 20.0 °C
1.010 BTU/lb-°F
@Temperature 68.0 °F
Thermal Conductivity 0.595 W/m-K
@Temperature 20.0 °C
4.13 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
liquid
 0.0270 W/m-K
@Pressure 0.100 MPa,
Temperature 127 °C
0.187 BTU-in/hr-ft²-°F
@Pressure 14.5 psi,
Temperature 260 °F
gas
 0.0365 W/m-K
@Pressure 0.100 MPa,
Temperature 227 °C
0.253 BTU-in/hr-ft²-°F
@Pressure 14.5 psi,
Temperature 440 °F
gas
 0.0476 W/m-K
@Pressure 0.100 MPa,
Temperature 327 °C
0.330 BTU-in/hr-ft²-°F
@Pressure 14.5 psi,
Temperature 620 °F
gas
Melting Point 3.82 °C38.9 °F
Boiling Point 101.42 °C214.56 °F
 
Descriptive Properties
Antoine's Vapor Pressure B Parameter0
Antoine's Vapor Pressure C Parameter0
CAS Number7789-20-0
Critical Compressibility (Zc)0.225
Dipole moment (p/C.m)6.338E-28
Molar Heat Capacity (298K)0 J/mol-K

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Elkem (Bluestar Silicones) BLUESIL™ FLD 47 V 3 Polydimethylsiloxanic Fluids
Water, H2O
Celanese 50000437 Acetic Anhydride
Overview - Alumina, 98%, Al2O3
PBI Performance Products S26 Thermal Resistant Polybenzimidazole Solution

DWATR1 / 99769

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.