MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Celanese Impet® 320R Recycled PET, 15% Glass Reinforced
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), Recycled, Glass Reinforced

Material Notes: General purpose, good mechanical properties.

Information provided by Celanese Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.43 g/cc0.0517 lb/in³ISO 1183
Water Absorption 0.10 %0.10 %ISO 62
Linear Mold Shrinkage, Flow 0.0025 cm/cm0.0025 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 8484ISO 2039
Tensile Strength, Ultimate 115 MPa16700 psiISO 527
Elongation at Break 3.0 %3.0 %ASTM D638
Flexural Strength 165 MPa23900 psiISO 178
Flexural Modulus 5.20 GPa754 ksiISO 178
Izod Impact, Notched 0.550 J/cm1.03 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 3.1
@Frequency 100000 Hz
3.1
@Frequency 100000 Hz
ASTM D150
Dielectric Strength 21.0 kV/mm
@Thickness 3.17 mm
533 kV/in
@Thickness 0.125 in
ASTM D149
Dissipation Factor 0.010
@Frequency 100000 Hz
0.010
@Frequency 100000 Hz
ASTM D150
Arc Resistance 119 sec119 secASTM D495
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  15.12 µm/m-°C
@Temperature 100 °C
8.400 µin/in-°F
@Temperature 212 °F
ASTM E831
 34.2 µm/m-°C
@Temperature 20.0 °C
19.0 µin/in-°F
@Temperature 68.0 °F
ASTM E831
CTE, linear, Transverse to Flow  46.8 µm/m-°C
@Temperature 100 °C
26.0 µin/in-°F
@Temperature 212 °F
ASTM E831
 76.0 µm/m-°C
@Temperature 20.0 °C
42.2 µin/in-°F
@Temperature 68.0 °F
ASTM E831
Melting Point 248 °C478 °FDSC; ISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 235 °C455 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 203 °C397 °FASTM D648
Flammability, UL94 HBHB
 
Processing PropertiesMetricEnglishComments
Processing Temperature 270 - 280 °C518 - 536 °FInjection; barrel center zone temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Ethylene Vinyl Alcohol (EVOH)
Celanese Impet® 610R Recycled PET, 13% Glass/Mineral Reinforced
Lotte Advanced Materials Starex® GC-0770 H ABS/PET, Unreinforced Recycled
MTM Plastics Dipolen® S Recycled PP + PE Blend
Polykemi AB SCANFILL Injection CPC15051 PP/PE, Mineral Reinforced

PHCU70 / 45810

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.