MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Impet® 320R Recycled PET, 15% Glass Reinforced
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), Recycled, Glass Reinforced

Material Notes: General purpose, good mechanical properties.

Information provided by Celanese Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.43 g/ccISO 1183
Water Absorption 0.10 %ISO 62
Linear Mold Shrinkage, Flow 0.0025 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 84ISO 2039
Tensile Strength, Ultimate 115 MPaISO 527
Elongation at Break 3.0 %ASTM D638
Flexural Strength 165 MPaISO 178
Flexural Modulus 5.20 GPaISO 178
Izod Impact, Notched 0.550 J/cmASTM D256
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 3.1
@Frequency 100000 Hz
ASTM D150
Dielectric Strength 21.0 kV/mm
@Thickness 3.17 mm
ASTM D149
Dissipation Factor 0.010
@Frequency 100000 Hz
ASTM D150
Arc Resistance 119 secASTM D495
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 15.12 µm/m-°C
@Temperature 100 °C
ASTM E831
 34.2 µm/m-°C
@Temperature 20.0 °C
ASTM E831
CTE, linear, Transverse to Flow 46.8 µm/m-°C
@Temperature 100 °C
ASTM E831
 76.0 µm/m-°C
@Temperature 20.0 °C
ASTM E831
Melting Point 248 °CDSC; ISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 235 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 203 °CASTM D648
Flammability, UL94 HB
 
Processing PropertiesOriginal ValueComments
Processing Temperature 270 - 280 °CInjection; barrel center zone temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Ethylene Vinyl Alcohol (EVOH)
Celanese Impet® 610R Recycled PET, 13% Glass/Mineral Reinforced
Lotte Advanced Materials Starex® GC-0770 H ABS/PET, Unreinforced Recycled
MTM Plastics Dipolen® S Recycled PP + PE Blend
Polykemi AB SCANFILL Injection CPC15051 PP/PE, Mineral Reinforced

PHCU70 / 45810

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.