MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Ascend Performance Materials Vydyne® 833C Nylon 66, Extrusion Grade  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Extruded; Nylon 66, Film

Material Notes: 833C is a PA66-based copolymer that features intermediate melt strength, shear thinning behavior, high tensile strength, ductility, and high clarity making it ideal for cast film applications. This material has ideal processability for cast film, oriented cast film (mono or biax), and profile/sheet/tubing extrusions. Specifically as an oriented film, it imparts extremely high strength and puncture resistance while maintaining a high elongation to break; further, depending on the annealing process, it can have tailored shrinkage from < 1% to > 20% making it appealing to a large number of end use film applications.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.674 g/cc0.0243 lb/in³ASTM D1895
Density 1.14 g/cc0.0412 lb/in³ISO 1183
Moisture Absorption 0.100 %0.100 %ASTM D6869
Viscosity Measurement 3.2 - 3.43.2 - 3.4Relative Viscosity - Sulfuric Acid; ISO 307
 75 - 9075 - 90Relative Viscosity - Formic Acid; ASTM D789
 
Mechanical PropertiesMetricEnglishComments
Puncture Resistance >= 2400 N
@Thickness 0.0250 mm
>= 540 lb (f)
@Thickness 0.000984 in
Cast Film, Conditioned; ASTM F1306
Film Tensile Strength at Yield, MD 31.0 MPa
@Thickness 0.0380 mm
4500 psi
@Thickness 0.00150 in
Cast Film, Conditioned; ASTM D882
Film Tensile Strength at Yield, TD 31.0 MPa
@Thickness 0.0380 mm
4500 psi
@Thickness 0.00150 in
Cast Film, Conditioned; ASTM D882
Film Elongation at Break, MD  130 %
@Thickness 0.0250 mm
130 %
@Thickness 0.000984 in
Cast Film, Conditioned; ASTM D882
 >= 450 %
@Thickness 0.0380 mm
>= 450 %
@Thickness 0.00150 in
Cast Film, Conditioned; ASTM D882
Film Elongation at Break, TD  130 %
@Thickness 0.0250 mm
130 %
@Thickness 0.000984 in
Cast Film, Conditioned; ASTM D882
 >= 500 %
@Thickness 0.0380 mm
>= 500 %
@Thickness 0.00150 in
Cast Film, Conditioned; ASTM D882
Film Elongation at Yield, MD 6.5 %
@Thickness 0.0380 mm
6.5 %
@Thickness 0.00150 in
Cast Film, Conditioned; ASTM D882
Film Elongation at Yield, TD 6.4 %
@Thickness 0.0380 mm
6.4 %
@Thickness 0.00150 in
Cast Film, Conditioned; ASTM D882
Secant Modulus, MD  0.601 GPa
@Thickness 0.0380 mm
87.2 ksi
@Thickness 0.00150 in
Cast Film, Conditioned; ASTM D882
 0.601 GPa
@Thickness 0.0380 mm
87.2 ksi
@Thickness 0.00150 in
Cast Film, Conditioned; ASTM D882
 3.31 GPa
@Thickness 0.0250 mm
480 ksi
@Thickness 0.000984 in
Cast Film, Conditioned; ASTM D882
Secant Modulus, TD  0.558 GPa
@Thickness 0.0380 mm
80.9 ksi
@Thickness 0.00150 in
Cast Film, Conditioned; ASTM D882
 0.558 GPa
@Thickness 0.0380 mm
80.9 ksi
@Thickness 0.00150 in
Cast Film, Conditioned; ASTM D882
 3.38 GPa
@Thickness 0.0250 mm
490 ksi
@Thickness 0.000984 in
Cast Film, Conditioned; ASTM D882
Elmendorf Tear Strength MD 71 g
@Thickness 0.0380 mm
71 g
@Thickness 0.00150 in
Cast Film, Conditioned; ASTM D1922
Elmendorf Tear Strength TD 91 g
@Thickness 0.0380 mm
91 g
@Thickness 0.00150 in
Cast Film, Conditioned; ASTM D1922
Dart Drop Test >= 2000 g
@Thickness 0.0380 mm
>= 4.41 lb
@Thickness 0.00150 in
Cast Film, Conditioned; ASTM D1709A
Film Tensile Strength at Break, MD  121 MPa
@Thickness 0.0380 mm
17500 psi
@Thickness 0.00150 in
Cast Film, Conditioned; ASTM D882
 280 MPa
@Thickness 0.0250 mm
40600 psi
@Thickness 0.000984 in
Cast Film, Conditioned; ASTM D882
Film Tensile Strength at Break, TD  101 MPa
@Thickness 0.0380 mm
14600 psi
@Thickness 0.00150 in
Cast Film, Conditioned; ASTM D882
 300 MPa
@Thickness 0.0250 mm
43500 psi
@Thickness 0.000984 in
Cast Film, Conditioned; ASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 235 °C455 °FISO 11357-3
Shrinkage, MD 0.90 %
@Treatment Temp. 160 °C,
Thickness 0.0250 mm
0.90 %
@Treatment Temp. 320 °F,
Thickness 0.000984 in
Cast Film, Conditioned; ASTM D1204
Shrinkage, TD 0.10 %
@Treatment Temp. 160 °C,
Thickness 0.0250 mm
0.10 %
@Treatment Temp. 320 °F,
Thickness 0.000984 in
Cast Film, Conditioned; ASTM D1204
 
Processing PropertiesMetricEnglishComments
Processing Temperature 20.0 - 40.0 °C68.0 - 104 °FBlow Film Air Temperature
 245 - 265 °C473 - 509 °FCylinder - Extrusion
Die Temperature 255 - 275 °C491 - 527 °FExtrusion
 70.0 - 80.0 °C
@Time 0.000 - 14400 sec
158 - 176 °F
@Time 0.000 - 4.00 hour
Extrusion
Melt Temperature 235 °C455 °FExtrusion
Moisture Content 0.030 - 0.080 %0.030 - 0.080 %Extrusion
 
Compliance PropertiesMetricEnglishComments
European Food 1935/2004 YesYes
 
Descriptive Properties
Agency RatingsEU 10/2011
 EU 2023/2006
FeaturesChemical Resistant
 Good melt strength
 High Melt Stability
 High Strength
 High Toughness
 Puncture resistant
Melt Pressure MPa3-17
Processing MethodCast Film
 Extrusion
 Profile extrusion
Screw DesignGP or Barrier
UsesIndustrial Applications
 Monofilaments
 Multilayer film
 Profiles
 Rods
 Sheet
 Tubing
 Vacuum Bagging Film

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ascend Performance Materials Vydyne® 833F Nylon 66, Extrusion Grade
Envalior Novamid® 2620A PA6/6T
EMS-Grivory Grivory® HB 5299 HV PA*
Domo Domamid® 33 Polyamide 6
Ascend Performance Materials Vydyne® 75HB NT0679 Nylon 66, Extrusion Grade

PZASCE9770 / 220873

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.