MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ascend Performance Materials Vydyne® 833F Nylon 66, Extrusion Grade  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Extruded; Nylon 66, Film

Material Notes: Vydyne 833F is a PA66-based copolymer that features good melt strength (ideal for cast film and certain blown film processes), shear thinning behavior, high tensile strength, ductility, and slow crystallinity that matches crystallization temperatures/rates very close to that of ethylenes. The combination of properties exhibited by Vydyne 833F make it a good candidate for a number of applications such as numerous film uses, sheeting, and monofilament. The slow crystallization behavior coupled with the melting point ~ 215-220°C and great mechanical properties makes this material extremely useful for outside layers or internal layers of the multilayer film. This material further exhibits a very high elongation to break (> 500%) allowing for high draw ratios for thermoforming or when orienting the film.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.674 g/cc0.0243 lb/in³ASTM D1895
Density 1.14 g/cc0.0412 lb/in³ISO 1183
Moisture Absorption 0.100 %0.100 %ASTM D6869
Viscosity Measurement 3.2 - 3.43.2 - 3.4Relative Viscosity - Sulfuric Acid; ISO 307
 75 - 9075 - 90Relative Viscosity - Formic Acid; ASTM D789
 
Mechanical PropertiesMetricEnglishComments
Puncture Resistance >= 2300 N
@Thickness 0.0250 mm
>= 517 lb (f)
@Thickness 0.000984 in
Cast Film, Conditioned; ASTM F1306
Film Elongation at Break, MD  140 %
@Thickness 0.0250 mm
140 %
@Thickness 0.000984 in
Cast Film, Conditioned; ASTM D882
 >= 500 %
@Thickness 0.0380 mm
>= 500 %
@Thickness 0.00150 in
Cast Film, Conditioned; ASTM D882
Film Elongation at Break, TD  130 %
@Thickness 0.0250 mm
130 %
@Thickness 0.000984 in
Cast Film, Conditioned; ASTM D882
 >= 500 %
@Thickness 0.0380 mm
>= 500 %
@Thickness 0.00150 in
Cast Film, Conditioned; ASTM D882
Film Elongation at Yield, MD 6.5 %
@Thickness 0.0380 mm
6.5 %
@Thickness 0.00150 in
Cast Film, Conditioned; ASTM D882
Film Elongation at Yield, TD 6.4 %
@Thickness 0.0380 mm
6.4 %
@Thickness 0.00150 in
Cast Film, Conditioned; ASTM D882
Secant Modulus, MD  0.400 GPa
@Thickness 0.0380 mm
58.0 ksi
@Thickness 0.00150 in
Cast Film, Conditioned; ASTM D882
 2.90 GPa
@Thickness 0.0250 mm
421 ksi
@Thickness 0.000984 in
Cast Film, Conditioned; ASTM D882
Secant Modulus, TD  0.400 GPa
@Thickness 0.0380 mm
58.0 ksi
@Thickness 0.00150 in
Cast Film, Conditioned; ASTM D882
 3.00 GPa
@Thickness 0.0250 mm
435 ksi
@Thickness 0.000984 in
Cast Film, Conditioned; ASTM D882
Elmendorf Tear Strength MD 140 g
@Thickness 0.0380 mm
140 g
@Thickness 0.00150 in
Cast Film, Conditioned; ASTM D1922
Elmendorf Tear Strength TD 154 g
@Thickness 0.0380 mm
154 g
@Thickness 0.00150 in
Cast Film, Conditioned; ASTM D1922
Dart Drop Test >= 2000 g
@Thickness 0.0380 mm
>= 4.41 lb
@Thickness 0.00150 in
Cast Film, Conditioned; ASTM D1709A
Film Tensile Strength at Break, MD 240 MPa
@Thickness 0.0250 mm
34800 psi
@Thickness 0.000984 in
Cast Film, Conditioned; ASTM D882
Film Tensile Strength at Break, TD 270 MPa
@Thickness 0.0250 mm
39200 psi
@Thickness 0.000984 in
Cast Film, Conditioned; ASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °FISO 11357-3
Shrinkage, MD 2.0 %
@Treatment Temp. 160 °C,
Thickness 0.0250 mm
2.0 %
@Treatment Temp. 320 °F,
Thickness 0.000984 in
Cast Film, Conditioned; ASTM D1204
Shrinkage, TD 1.0 %
@Treatment Temp. 160 °C,
Thickness 0.0250 mm
1.0 %
@Treatment Temp. 320 °F,
Thickness 0.000984 in
Cast Film, Conditioned; ASTM D1204
 
Processing PropertiesMetricEnglishComments
Processing Temperature 5.00 - 20.0 °C41.0 - 68.0 °FBlow Film Air Temperature
 230 - 270 °C446 - 518 °FCylinder - Extrusion
Die Temperature 240 °C464 °FExtrusion
 70.0 - 80.0 °C
@Time 0.000 - 14400 sec
158 - 176 °F
@Time 0.000 - 4.00 hour
Extrusion
Melt Temperature 220 °C428 °FExtrusion
Moisture Content 0.030 - 0.080 %0.030 - 0.080 %Extrusion
 
Compliance PropertiesMetricEnglishComments
European Food 1935/2004 YesYes
FDA YesYes21CFR 177.1500
 
Descriptive Properties
Agency RatingsASTM D 4066 PA0111
 ASTM D 6779 PA0111
 EU 10/2011
 EU 2023/2006
 MIL M-20693B
 NSF STD-51
FeaturesGood Chemical Resistance
 High Melt Stability
 High melt strength
 High Strength
 High Toughness
 Puncture resistant
Melt Pressure MPa3-17
Screw DesignGP or Barrier
UsesIndustrial Applications
 Monofilaments
 Multilayer film
 Profiles
 Rods
 Sheet
 Tubing
 Vacuum Bagging Film

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ascend Performance Materials Vydyne® 833C Nylon 66, Extrusion Grade
Envalior Novamid® 2620A PA6/6T
EMS-Grivory Grivory® HB 5299 HV PA*
Domo Domamid® 33 Polyamide 6
Ascend Performance Materials Vydyne® 75HB NT0679 Nylon 66, Extrusion Grade

PZASCE9771 / 220874

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.