MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

A. Schulman BMC G10(12) Mineral Filled, Glass Fiber Reinforced Polyester
Categories: Polymer; Thermoset; Polyester, TS; Thermoset Polyester Glass and Mineral Filled BMC

Material Notes: BMC G10 is a general purpose, mineral filled, glass fiber-reinforced polyester that is suitable for compression, transfer and stuffer injection molding. G10 is well suited to applications where high surface hardness is required.

Information provided by Bulk Molding Compounds, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.07 - 2.27 g/cc0.0748 - 0.0820 lb/in³Molded
Linear Mold Shrinkage 0.0022 - 0.0042 cm/cm0.0022 - 0.0042 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Barcol 60 - 7060 - 70
Tensile Strength 49.6 - 63.4 MPa7200 - 9200 psi
Flexural Strength 103 - 131 MPa15000 - 19000 psi
Flexural Modulus 7.58 - 8.96 GPa1100 - 1300 ksi
Compressive Strength 135 - 163 MPa19600 - 23600 psi
Izod Impact, Notched 2.30 - 2.40 J/cm4.30 - 4.50 ft-lb/in
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 13.2 - 15.2 kV/mm335 - 385 kV/inshort time
Arc Resistance 181 sec181 sec
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 218 - 260 °C425 - 500 °F
Flammability, UL94 HBHB
 
Processing PropertiesMetricEnglishComments
Processing Temperature 143 - 171 °C290 - 340 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
G-10 Fiberglass Epoxy Laminate Sheet
Nickel, Ni
A. Schulman BMC 610 Mineral filled, glass-fiber-reinforced polyester compound
A. Schulman BMC Super-Tough Mineral Filled, Glass Reinforced Polyester
A. Schulman BMC T40-4020-AQ High Strength Arc Quenching Molding Compound

PBMC916 / 123380

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.