Hyflon® MFA is a family of perfluoro polymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, high flexural endurance, inherent flame resistance, low surface energy and exceptional dielectric properties. Hyflon® MFA F1530 is a medium-low melt flow rate multi purpose resin with an exceptional stress crack resistance, continuous service temperature up to 225°C and a 40-60x10³ cycles flex life (on a 0.3 mm film, ASTM D2176). Features: Flame Retardant; High ESCR (Stress Crack Resist.); Medium Flow Uses: General Purpose; Wire & Cable Applications Additional Properties: Crystallization Heat - DSC 16.0 to 24.0 J/g; Flange Temperature - 370 to 400 °C; Flex Life - ASTM D2176 4.0E+4 to 6.0E+4 Cycles; Heat of Fusion - DSC 16.0 to 24.0 J/g Information provided by Solvay Specialty Polymers. |