MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Syensqo (Solvay Specialty Polymers) Hyflon® P6010 Perfluoropolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Fluoropolymer

Material Notes: Hyflon® MFA P6010 is a clear, semi-crystalline melt processable perfluorinated resin. It is designed for electrostatic powder coatings and is particularly recommended for use as a topcoat in antistick applications.

Hyflon® MFA P6010 exhibits very low surface energy, very low coefficient of friction, excellent optical properties and outstanding thermal and flame resistance. Additionally Hyflon® MFA P6010 coatings show excellent smooth surface finish, optimum antistick behavior and can maintain performance over a wide temperature range.

Main features of Hyflon® MFA P6010 include:

- Optimum antistick behavior

- Very low coefficient of friction

- Excellent surface finish

- Excellent thermal resistance

Good Optical Properties; Good Surface Finish; Good Thermal Stability; Low Friction; Semi Crystalline

Uses: Coating Applications

Processing: Coating

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.16 g/cc2.16 g/ccASTM D792
Particle Size 25 µm25 µm
Melt Flow 10 - 17 g/10 min
@Load 5.00 kg,
Temperature 372 °C
10 - 17 g/10 min
@Load 11.0 lb,
Temperature 702 °F
ASTM D1238
 
Thermal PropertiesMetricEnglishComments
Melting Point 280 - 290 °C536 - 554 °F
 
Descriptive Properties
ColorClear/Transparent
FormsPowder

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Syensqo (Solvay Specialty Polymers) Hyflon® MFA® F1530 Perfluoropolymer
Syensqo (Solvay Specialty Polymers) Hyflon® PFA P120X Perfluoroalkoxy (PFA)
Syensqo (Solvay Specialty Polymers) Hyflon® PFA C920-0020X Perfluoroalkoxy (PFA)
Syensqo (Solvay Specialty Polymers) Hyflon® PFA 450 Fluoropolymer
Syensqo (Solvay Specialty Polymers) Hyflon® F1540 Perfluoropolymer

PSOL8Y6218 / 193139

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.