MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Overview of materials for Nylon 6, 40% Glass Fiber Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 40% Glass Fiber Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.30 - 1.75 g/cc0.0470 - 0.0632 lb/in³Average value: 1.44 g/cc Grade Count:390
 1.23 - 1.33 g/cc
@Temperature 220 - 325 °C
0.0444 - 0.0480 lb/in³
@Temperature 428 - 617 °F
Average value: 1.27 g/cc Grade Count:5
Filler Content 33.0 - 44.0 %33.0 - 44.0 %Average value: 39.0 % Grade Count:57
Water Absorption 0.200 - 7.10 %0.200 - 7.10 %Average value: 2.72 % Grade Count:163
Moisture Absorption at Equilibrium 0.250 - 6.20 %0.250 - 6.20 %Average value: 1.91 % Grade Count:122
 1.50 - 2.10 %
@Temperature 70.0 - 70.0 °C
1.50 - 2.10 %
@Temperature 158 - 158 °F
Average value: 1.82 % Grade Count:14
Water Absorption at Saturation 3.50 - 7.50 %3.50 - 7.50 %Average value: 5.67 % Grade Count:96
Additive Loading 40.0 %40.0 %Average value: 40.0 % Grade Count:5
Viscosity 2.60 - 50.0 cP2.60 - 50.0 cPAverage value: 12.2 cP Grade Count:5
 30.0 - 1000 cP
@Temperature 240 - 280 °C
30.0 - 1000 cP
@Temperature 464 - 536 °F
Average value: 286 cP Grade Count:2
 30.0 - 1000 cP
@Shear Rate 100 - 10000 1/s
30.0 - 1000 cP
@Shear Rate 100 - 10000 1/s
Average value: 286 cP Grade Count:2
Viscosity Test 145 - 150 cm³/g1.45 - 1.50 dl/gAverage value: 146 cm³/g Grade Count:7
Viscosity Number 100 - 150 cm³/g1.00 - 1.50 dl/gAverage value: 136 cm³/g Grade Count:7
Maximum Moisture Content 0.0200 - 0.2000.0200 - 0.200Average value: 0.132 Grade Count:16
 0.300 - 0.300
@Temperature 120 - 120 °C
0.300 - 0.300
@Temperature 248 - 248 °F
Average value: 0.300 Grade Count:1
 0.300 - 0.300
@Time 299 - 299 sec
0.300 - 0.300
@Time 0.0830 - 0.0830 hour
Average value: 0.300 Grade Count:1
Linear Mold Shrinkage 0.000300 - 0.0350 cm/cm0.000300 - 0.0350 in/inAverage value: 0.00378 cm/cm Grade Count:287
 0.00200 - 0.00300 cm/cm
@Temperature 80.0 - 80.0 °C
0.00200 - 0.00300 in/in
@Temperature 176 - 176 °F
Average value: 0.00233 cm/cm Grade Count:6
Linear Mold Shrinkage, Transverse 0.000700 - 0.0590 cm/cm0.000700 - 0.0590 in/inAverage value: 0.00706 cm/cm Grade Count:154
 0.00700 - 0.00700 cm/cm
@Temperature 80.0 - 80.0 °C
0.00700 - 0.00700 in/in
@Temperature 176 - 176 °F
Average value: 0.00700 cm/cm Grade Count:6
Melt Flow 1.00 - 78.7 g/10 min1.00 - 78.7 g/10 minAverage value: 26.4 g/10 min Grade Count:39
Spiral Flow 48.0 - 610 cm18.9 - 240 inAverage value: 174 cm Grade Count:9
Ash 38.0 - 46.0 %38.0 - 46.0 %Average value: 41.5 % Grade Count:6
 58.0 - 62.0 %
@Temperature 625 - 625 °C
58.0 - 62.0 %
@Temperature 1160 - 1160 °F
Average value: 60.0 % Grade Count:1
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 88.0 - 10888.0 - 108Average value: 94.0 Grade Count:9
Hardness, Rockwell R 109 - 124109 - 124Average value: 121 Grade Count:47
Hardness, Shore D 77.0 - 84.077.0 - 84.0Average value: 80.2 Grade Count:3
Ball Indentation Hardness 84.0 - 310 MPa12200 - 45000 psiAverage value: 204 MPa Grade Count:53
Tensile Strength, Ultimate 65.0 - 470 MPa9430 - 68200 psiAverage value: 167 MPa Grade Count:334
 77.0 - 281.306 MPa
@Temperature -40.0 - 150 °C
11200 - 40800.1 psi
@Temperature -40.0 - 302 °F
Average value: 114 MPa Grade Count:4
 40.0 - 160 MPa
@Temperature 60.0 - 150 °C
5800 - 23200 psi
@Temperature 140 - 302 °F
Average value: 114 MPa Grade Count:1
 40.0 - 160 MPa
@Strain 1.00 - 3.00 %
5800 - 23200 psi
@Strain 1.00 - 3.00 %
Average value: 114 MPa Grade Count:1
Tensile Strength, Yield 74.0 - 234 MPa10700 - 34000 psiAverage value: 178 MPa Grade Count:63
Elongation at Break 1.00 - 11.0 %1.00 - 11.0 %Average value: 3.70 % Grade Count:353
 2.60 - 7.00 %
@Temperature -40.0 - 150 °C
2.60 - 7.00 %
@Temperature -40.0 - 302 °F
Average value: 4.99 % Grade Count:4
Elongation at Yield 2.00 - 9.50 %2.00 - 9.50 %Average value: 3.64 % Grade Count:24
Modulus of Elasticity 4.60 - 15.9 GPa667 - 2300 ksiAverage value: 10.2 GPa Grade Count:263
 3.70 - 12.0 GPa
@Temperature -40.0 - 150 °C
537 - 1740 ksi
@Temperature -40.0 - 302 °F
Average value: 7.97 GPa Grade Count:3
Flexural Yield Strength 97.2 - 370 MPa14100 - 53700 psiAverage value: 244 MPa Grade Count:256
 138 - 450 MPa
@Temperature -40.0 - 121 °C
20000 - 65300 psi
@Temperature -40.0 - 250 °F
Average value: 249 MPa Grade Count:5
Flexural Modulus 1.18 - 13.8 GPa171 - 2000 ksiAverage value: 9.40 GPa Grade Count:290
 4.83 - 12.4795 GPa
@Temperature -40.0 - 121 °C
701 - 1810.03 ksi
@Temperature -40.0 - 250 °F
Average value: 6.81 GPa Grade Count:5
Flexural Strain at Break 3.40 - 6.00 %3.40 - 6.00 %Average value: 4.65 % Grade Count:25
Compressive Yield Strength 149 - 258 MPa21600 - 37400 psiAverage value: 187 MPa Grade Count:11
Poissons Ratio 0.330 - 0.3500.330 - 0.350Average value: 0.337 Grade Count:18
Shear Modulus 4.60 - 5.00 GPa667 - 725 ksiAverage value: 4.73 GPa Grade Count:3
Shear Strength 60.0 - 77.2 MPa8700 - 11200 psiAverage value: 71.4 MPa Grade Count:3
Izod Impact, Notched 0.140 - 13.2 J/cm0.262 - 24.8 ft-lb/inAverage value: 1.63 J/cm Grade Count:109
 0.0800 - 5.12544 J/cm
@Temperature -40.0 - 121 °C
0.150 - 9.60205 ft-lb/in
@Temperature -40.0 - 250 °F
Average value: 1.59 J/cm Grade Count:2
 0.74746 - 1.28136 J/cm
@Temperature -40.0 - -40.0 °C
1.4003 - 2.40051 ft-lb/in
@Temperature -40.0 - -40.0 °F
Average value: 1.59 J/cm Grade Count:3
 0.74746 - 1.28136 J/cm
@Thickness 3.17 - 3.17 mm
1.4003 - 2.40051 ft-lb/in
@Thickness 0.125 - 0.125 in
Average value: 1.59 J/cm Grade Count:3
Izod Impact, Unnotched 0.770 - 14.4 J/cm1.44 - 27.0 ft-lb/inAverage value: 10.4 J/cm Grade Count:37
 0.710 - 0.750 J/cm
@Temperature -30.0 - -30.0 °C
1.33 - 1.41 ft-lb/in
@Temperature -22.0 - -22.0 °F
Average value: 0.730 J/cm Grade Count:2
Izod Impact, Notched (ISO) 7.00 - 79.0 kJ/m²3.33 - 37.6 ft-lb/in²Average value: 18.4 kJ/m² Grade Count:123
 8.00 - 18.0 kJ/m²
@Temperature -40.0 - -30.0 °C
3.81 - 8.57 ft-lb/in²
@Temperature -40.0 - -22.0 °F
Average value: 12.2 kJ/m² Grade Count:40
Izod Impact, Unnotched (ISO) 24.0 - 110 kJ/m²11.4 - 52.3 ft-lb/in²Average value: 75.7 kJ/m² Grade Count:35
 18.0 - 95.0 kJ/m²
@Temperature -30.0 - -30.0 °C
8.57 - 45.2 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 64.9 kJ/m² Grade Count:19
Charpy Impact Unnotched 3.50 J/cm² - NB16.7 ft-lb/in² - NBAverage value: 8.92 J/cm² Grade Count:209
 3.30 J/cm² - NB
@Temperature -40.0 - -20.0 °C
15.7 ft-lb/in² - NB
@Temperature -40.0 - -4.00 °F
Average value: 7.81 J/cm² Grade Count:135
Charpy Impact, Notched 0.380 - 11.7 J/cm²1.81 - 55.4 ft-lb/in²Average value: 1.91 J/cm² Grade Count:246
 0.370 - 11.0 J/cm²
@Temperature -40.0 - -20.0 °C
1.76 - 52.4 ft-lb/in²
@Temperature -40.0 - -4.00 °F
Average value: 1.29 J/cm² Grade Count:125
Puncture Energy 2.30 - 9.10 J1.70 - 6.71 ft-lbAverage value: 5.31 J Grade Count:6
 1.60 - 6.00 J
@Temperature -30.0 - -30.0 °C
1.18 - 4.43 ft-lb
@Temperature -22.0 - -22.0 °F
Average value: 3.78 J Grade Count:5
Tensile Creep Modulus, 1 hour 6000 - 11000 MPa870000 - 1.60e+6 psiAverage value: 7690 MPa Grade Count:7
Tensile Creep Modulus, 1000 hours 3300 - 9500 MPa479000 - 1.38e+6 psiAverage value: 5990 MPa Grade Count:14
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+6 - 1.00e+18 ohm-cm1.00e+6 - 1.00e+18 ohm-cmAverage value: 6.53e+15 ohm-cm Grade Count:179
 1.00e+8 - 1.00e+16 ohm-cm
@Temperature 40.0 - 140 °C
1.00e+8 - 1.00e+16 ohm-cm
@Temperature 104 - 284 °F
Average value: 1.46e+15 ohm-cm Grade Count:2
Surface Resistance 1e+05 - 1.00e+16 ohm1e+05 - 1.00e+16 ohmAverage value: 1.62e+14 ohm Grade Count:108
Dielectric Constant 1.50 - 15.01.50 - 15.0Average value: 5.39 Grade Count:80
Dielectric Strength 7.87 - 80.0 kV/mm200 - 2030 kV/inAverage value: 29.4 kV/mm Grade Count:113
Dissipation Factor 0.00500 - 0.3000.00500 - 0.300Average value: 0.0773 Grade Count:72
Comparative Tracking Index 275 - 600 V275 - 600 VAverage value: 533 V Grade Count:124
 
Thermal PropertiesMetricEnglishComments
CTE, linear 7.00 - 60.0 µm/m-°C3.89 - 33.3 µin/in-°FAverage value: 22.4 µm/m-°C Grade Count:100
 13.0 - 18.0 µm/m-°C
@Temperature 55.0 - 160 °C
7.22 - 10.0 µin/in-°F
@Temperature 131 - 320 °F
Average value: 19.1 µm/m-°C Grade Count:4
 21.0 - 21.0 µm/m-°C
@Temperature 35.0 - 55.0 °C
11.7 - 11.7 µin/in-°F
@Temperature 95.0 - 131 °F
Average value: 19.1 µm/m-°C Grade Count:3
 21.0 - 21.0 µm/m-°C
@Thickness 2.00 - 2.00 mm
11.7 - 11.7 µin/in-°F
@Thickness 0.0787 - 0.0787 in
Average value: 19.1 µm/m-°C Grade Count:3
CTE, linear, Transverse to Flow 15.0 - 140 µm/m-°C8.33 - 77.8 µin/in-°FAverage value: 67.5 µm/m-°C Grade Count:74
 66.0 - 80.0 µm/m-°C
@Temperature 55.0 - 160 °C
36.7 - 44.4 µin/in-°F
@Temperature 131 - 320 °F
Average value: 73.7 µm/m-°C Grade Count:3
Specific Heat Capacity 1.30 - 2.52 J/g-°C0.311 - 0.603 BTU/lb-°FAverage value: 1.63 J/g-°C Grade Count:9
 1.86 - 2.10 J/g-°C
@Temperature 270 - 325 °C
0.445 - 0.502 BTU/lb-°F
@Temperature 518 - 617 °F
Average value: 2.02 J/g-°C Grade Count:3
Thermal Conductivity 0.280 - 0.490 W/m-K1.94 - 3.40 BTU-in/hr-ft²-°FAverage value: 0.345 W/m-K Grade Count:21
 0.250 - 0.280 W/m-K
@Temperature 270 - 325 °C
1.74 - 1.94 BTU-in/hr-ft²-°F
@Temperature 518 - 617 °F
Average value: 0.263 W/m-K Grade Count:3
Melting Point 210 - 325 °C410 - 617 °FAverage value: 227 °C Grade Count:242
Maximum Service Temperature, Air 90.0 - 270 °C194 - 518 °FAverage value: 163 °C Grade Count:52
Deflection Temperature at 0.46 MPa (66 psi) 195 - 284 °C383 - 543 °FAverage value: 219 °C Grade Count:149
Deflection Temperature at 1.8 MPa (264 psi) 102 - 280 °C216 - 536 °FAverage value: 211 °C Grade Count:275
Deflection Temperature at 8.0 MPa 120 - 200 °C248 - 392 °FAverage value: 160 °C Grade Count:33
Vicat Softening Point 200 - 290 °C392 - 554 °FAverage value: 211 °C Grade Count:44
Glass Transition Temp, Tg 15.0 - 135 °C59.0 - 275 °FAverage value: 58.9 °C Grade Count:7
Decomposition Temperature 300 - 350 °C572 - 662 °FAverage value: 325 °C Grade Count:12
UL RTI, Electrical 120 - 140 °C248 - 284 °FAverage value: 136 °C Grade Count:7
UL RTI, Mechanical with Impact 90.0 - 125 °C194 - 257 °FAverage value: 114 °C Grade Count:7
UL RTI, Mechanical without Impact 130 - 150 °C266 - 302 °FAverage value: 141 °C Grade Count:7
Flammability, UL94 HB - 5VBHB - 5VBGrade Count:173
Flame Spread 0.000 - 102 mm/min0.000 - 4.02 in/minAverage value: 41.4 mm/min Grade Count:16
Oxygen Index 22.0 - 27.0 %22.0 - 27.0 %Average value: 23.8 % Grade Count:18
Glow Wire Test 550 - 750 °C1020 - 1380 °FAverage value: 654 °C Grade Count:35
Ignition Temperature 400 - 470 °C752 - 878 °FAverage value: 435 °C Grade Count:12
 
Processing PropertiesMetricEnglishComments
Processing Temperature 70.0 - 288 °C158 - 550 °FAverage value: 179 °C Grade Count:32
Nozzle Temperature 230 - 299 °C446 - 570 °FAverage value: 270 °C Grade Count:32
Melt Temperature 216 - 370 °C420 - 698 °FAverage value: 275 °C Grade Count:192
Mold Temperature 26.7 - 180 °C80.0 - 356 °FAverage value: 88.5 °C Grade Count:200
Injection Velocity 30.0 - 76.2 mm/sec1.18 - 3.00 in/secAverage value: 56.2 mm/sec Grade Count:3
Drying Temperature 65.6 - 180 °C150 - 356 °FAverage value: 85.1 °C Grade Count:153
Moisture Content 0.0300 - 0.200 %0.0300 - 0.200 %Average value: 0.144 % Grade Count:88
Dew Point -28.9 - -17.8 °C-20.0 - 0.000 °FAverage value: -18.9 °C Grade Count:10
Injection Pressure 3.45 - 138 MPa500 - 20000 psiAverage value: 71.5 MPa Grade Count:32

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Nylon 6, 30% Glass Fiber Filled
Overview of materials for Nylon 6, 50% Glass Fiber Filled
Overview of materials for Nylon 6, 20% Glass Fiber Filled
Overview of materials for Nylon 6, 10% Glass Fiber Filled
Overview of materials for Nylon 6, Unreinforced

O2414 / 77974

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.