MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Borealis FG5224 Linear Low Density Polyethylene
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade

Material Notes: FG5224 is a Butene Linear Low Density Polyethylene for Film Extrusion. Includes antioxidant, anti-block and medium slip additives. This grade is developed for production of lamination film. FG5224 has good heat sealing properties and hot tack strength. By mixing with FG5223 any desired level of friction can be obtained. Applications FG5224 has been developed especially for applications like: lamination films, shrink film, carrier-bag film, and food wrap film.

Information provided by Borealis AG

Key Words: LLDPE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.922 g/cc0.0333 lb/in³ISO 1183
Melt Flow 0.90 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.90 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Antiblock Level 625 ppm625 ppmBorealis Method
Slip Level 480 ppm480 ppmerucamide; Borealis Method
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 12.0 MPa1740 psiMD/TD; ISO 527-3
Film Elongation at Break, MD 800 %800 %ISO 527-3
Film Elongation at Break, TD 1000 %1000 %ISO 527-3
Tensile Modulus 0.145 GPa21.0 ksiMD; ASTM D882-A
 0.165 GPa23.9 ksiTD; ASTM D882-A
Coefficient of Friction, Dynamic 0.100.10ISO 8295
Elmendorf Tear Strength, MD 2.91 g/micron73.9 g/milISO 6383/2
Elmendorf Tear Strength, TD 13.11 g/micron333.0 g/milISO 6383/2
Dart Drop Test 260 g
@Thickness 0.0700 mm
0.573 lb
@Thickness 0.00276 in
ISO 7765-1
Film Tensile Strength at Break, MD 29.0 MPa4210 psiISO 527-3
Film Tensile Strength at Break, TD 28.0 MPa4060 psiISO 527-3
 
Thermal PropertiesMetricEnglishComments
Melting Point 122 °C252 °FISO 11357-3
 
Optical PropertiesMetricEnglishComments
Haze 10 %10 %ASTM D1003
Gloss 100 %100 %ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis FG5223 Linear Low Density Polyethylene
Borealis Borstar® FB2230 LLDPE for Film
Borealis FG5190 Linear Low Density Polyethylene
Borealis FG5199 Linear Low Density Polyethylene
Bamberger Polymers Bapolene® 222B Polyethylene Film Grade

PBOREA442 / 108701

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.