MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Borealis FG5224 Linear Low Density Polyethylene
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade

Material Notes: FG5224 is a Butene Linear Low Density Polyethylene for Film Extrusion. Includes antioxidant, anti-block and medium slip additives. This grade is developed for production of lamination film. FG5224 has good heat sealing properties and hot tack strength. By mixing with FG5223 any desired level of friction can be obtained. Applications FG5224 has been developed especially for applications like: lamination films, shrink film, carrier-bag film, and food wrap film.

Information provided by Borealis AG

Key Words: LLDPE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.922 g/ccISO 1183
Melt Flow 0.90 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
Antiblock Level 625 ppmBorealis Method
Slip Level 480 ppmerucamide; Borealis Method
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 12.0 MPaMD/TD; ISO 527-3
Film Elongation at Break, MD 800 %ISO 527-3
Film Elongation at Break, TD 1000 %ISO 527-3
Tensile Modulus 145 MPaMD; ASTM D882-A
 165 MPaTD; ASTM D882-A
Coefficient of Friction, Dynamic 0.10ISO 8295
Elmendorf Tear Strength, MD 2.91 g/micronISO 6383/2
Elmendorf Tear Strength, TD 13.11 g/micronISO 6383/2
Dart Drop Test 260 g
@Thickness 0.0700 mm
ISO 7765-1
Film Tensile Strength at Break, MD 29.0 MPaISO 527-3
Film Tensile Strength at Break, TD 28.0 MPaISO 527-3
 
Thermal PropertiesOriginal ValueComments
Melting Point 122 °CISO 11357-3
 
Optical PropertiesOriginal ValueComments
Haze 10 %ASTM D1003
Gloss 100 %ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borealis FG5223 Linear Low Density Polyethylene
Borealis Borstar® FB2230 LLDPE for Film
Borealis FG5190 Linear Low Density Polyethylene
Borealis FG5199 Linear Low Density Polyethylene
Bamberger Polymers Bapolene® 222B Polyethylene Film Grade

PBOREA442 / 108701

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.