MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hydrogen Sulfide, H2S
Categories: Ceramic; Sulfide/Chalcogenide; Fluid

Material Notes: Colorless flammable gas. Rotten egg smell, very toxic.

Key Words: H2S
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.001393 g/cc0.00005033 lb/in³Gas
Molecular Weight 34.076 g/mol34.076 g/mol
 34.081 g/mol34.081 g/mol
 
Electrical PropertiesMetricEnglishComments
Magnetic Susceptibility -0.0000255-0.0000255cm^3/mol
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 69.8 J/g30.0 BTU/lb
Thermal Conductivity  0.0146 W/m-K
@Pressure 0.100 MPa,
Temperature 26.9 °C
0.101 BTU-in/hr-ft²-°F
@Pressure 14.5 psi,
Temperature 80.3 °F
gas
 0.0205 W/m-K
@Pressure 0.100 MPa,
Temperature 127 °C
0.142 BTU-in/hr-ft²-°F
@Pressure 14.5 psi,
Temperature 260 °F
gas
 0.0264 W/m-K
@Pressure 0.100 MPa,
Temperature 227 °C
0.183 BTU-in/hr-ft²-°F
@Pressure 14.5 psi,
Temperature 440 °F
gas
 0.0324 W/m-K
@Pressure 0.100 MPa,
Temperature 327 °C
0.225 BTU-in/hr-ft²-°F
@Pressure 14.5 psi,
Temperature 620 °F
gas
Melting Point -85.5 °C-122 °F
Boiling Point -59.55 °C-75.19 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index  1.3682
@Temperature 20.0 °C,
Wavelength 589 nm
1.3682
@Temperature 68.0 °F,
Wavelength 589 nm
Liquid at Staurated Vapor Pressure
 1.460
@Temperature -80.0 °C,
Wavelength 589 nm
1.460
@Temperature -112 °F,
Wavelength 589 nm
Liquid
 
Descriptive Properties
CAS Number7783-06-4

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Cordierite, 2MgO-2Al2O3-5SiO2
ExxonMobil Varsol™ 120 Non-dearomatized Fluid
Solvay ALKAMIDE® AJ58BN Surfactant
Special Metals MONEL® Alloy 450
Special Metals MONEL® Alloy K-500

EINOR0320 / 3449

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.