MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Zinc Germanium Phosphide Arsenide, ZnGeP1.8As0.2
Categories: Ceramic; Phosphide/Pnictide

Material Notes:

Key Words: ZnGeP1.8As0.2
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
a Lattice Constant 5.48 Å5.48 Å
c Lattice Constant 10.742 Å10.742 Å
 
Mechanical PropertiesMetricEnglishComments
Knoop Microhardness 510510kg/mm²; 100 g indenter
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 2.50e+6 ohm-cm2.50e+6 ohm-cm
Band Gap 1.78 eV1.78 eV
 
Thermal PropertiesMetricEnglishComments
Decomposition Temperature 475 °C887 °FStability limit in flowing oxygen
 
Descriptive Properties
Crystal StructureTetragonalChalcopyrite Structure - Space Group I(-4)2d

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Zinc, Zn
Zinc Scandium Sulfide, ZnSc2S4
Aremco Ceramacast™ 589 High Temperature Potting & Casting Material Silica
COI Ceramics Nextel™ AS-N312 Oxide Ceramic Matrix Composite, Aluminosilicate
Mateck Zinc Sulphide, ZnS

BPHO01 / 286

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.