MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Specialty Compounds RTP Company
Quaker Quintolubric® 818-02 Longwall Roof Support
Categories: Fluid

Material Notes: Benefits:
  • Approved by Caterpillar, Inbye and other major OEMs at 2% in various minespecific waters
  • Approved by Joy at 2% in all water types, including type 19 (750 ppm)
  • Produced globally in ISO approved facilities to meet mining industry needs
  • 97.6% biodegradable in accordance with ISO 7827
  • Compatible at 2% with all commonly used longwall fluids for easy conversion
  • Optional dye for easy underground leak detection, and can help identify fluid injection in workers should an injection occur
Applications: QUINTOLUBRIC® 818-02 is a full solution synthetic, high water-based (HFA) hydraulic fluid concentrate designed for use in longwall shields. This fully synthetic concentrate has been specially engineered to pass the severe tests developed by Caterpillar, Joy and other major longwall shield OEMs.

Information provided by Quaker

Vendors:
Available Properties
  • Density, ASTM D287
  • pH, ASTM D70
  • Viscosity Measure, ASTM D445
  • Storage Temperature
  • Melting Point, ASTM D97, Freezing Point
  • Pour Point, ASTM D97
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Master Bond adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.