| Hifax TYC 1152PHS YZ9A Black is a very high melt flow, high flexural modulus, low density and high shrink mineral filled thermoplastic elastomeric olefin (TEO) resin that enables part weight reduction and associated savings while maintaining all of the performance of traditional, higher density products. It has an excellent balance of properties and processability, and is typically used for automotive bumper fascias and exterior trim applications. Availability: North America Application: Automotive Parts; Bumpers; Exterior Automotive Applications Market: Automotive Processing Method: Injection Molding Attribute: Good Dimensional Stability; Good Processability; High Impact Resistance; High Shrinkage; High Stiffness; Low Density Information provided by LyondellBasell. |