MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Elkem (Bluestar Silicones) SILCOLAPSE® 621 Silicone Antifoam Emulsion
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: SILCOLAPSE® 623 and SILCOLAPSE® 621 are water soluble defoamers designed for use in a wide range of aqueous industrial applications. SILCOLAPSE® 623 and SILCOLAPSE® 621 are 30% and 10% emulsions respectively formulated using Silcolapse 610 as the active defoaming silicone compound. These products effectively control foam at concentrations as low as 10 ppm solids, even at elevated temperatures and under pressure. SILCOLAPSE® 623 and SILCOLAPSE® 621 give good results at wide-ranging pH and are particularly effective in alkaline conditions.

Applications:

  • Industrial: Starch production; Soap and industrial detergent manufacturing; Metal working an cutting oils
  • Petroleum Refining: Gas scrubbing; Cement & Drilling muds; Asphalt production
  • Synthetic Rubber Processing: Natural or synthetic latex
  • Waste Water Treatment
  • Sea Water Distillation
  • Paints, Inks and Varnishes: Manufacture of aqueous pigments in alkaline pH
  • Pesticides: Insecticides, fungicides & herbicides; Glues, pastes and adhesives
  • Textiles: Sizing and Bleaching; High Temperature Dyeing; Finishing
Features:
  • Easy to use – as supplied or pre-diluted in water or in the medium to be defoamed
  • Cost efficient, effective in doses as low as 10 ppm
  • Highly effective in most aqueous media, and at many pH levels
  • Chemically inert in foaming systems – will not alter the properties of the foaming medium
  • Heat resistant – withstands temperatures up to 120°C (248°F)
  • Low viscosity allows it to be used with automatic metering systems

Information provided by Bluestar Silicones

Vendors:
Available Properties
  • Specific Gravity
  • pH
  • Viscosity
  • Storage Temperature
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.