MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Total PPR Z9421 Polypropylene, Random Copolymer, Heat Sealable Film Grade
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Color/Clarity/Impact. TOTAL Petrochemicals Polypropylene Z9421 is a low melting, high ethylene random copolymer with improved color, optics and impact properties.

Heat Sealable. The very low melting point of Z9421 makes it an excellent heat seal layer for oriented films.

FDA. Z9421 complies with all applicable FDA regulations Title 21 CFR Section 177.1520(c) 3.1 and may be used under these provisions for food contact and packaging.

Recommended Applications. Z9421 is recommended for use in non-oriented film processes for manufacture of films that require improved optical and impact properties and as a heat seal layer for oriented films.

Information provided by Total Petrochemicals.

Vendors:
Available Properties
  • Specific Gravity, ASTM D1505
  • Water Vapor Transmission, ASTM F1249-90, 90% RH
  • Melt Flow, ASTM D1238
  • Tensile Strength at Break, ASTM D882, non-oriented film
  • Elongation at Break, ASTM D882
  • Dart Drop, ASTM D1709
  • Heat Seal Strength Initiation Temperature
  • Melting Point, DSC
  • Haze, ASTM D1003
  • Gloss, ASTM D2457, at 45°
  • Melt Temperature
  • FDA, See notes for details.
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Total Atofina

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.