MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Solvay CYCOM® PR 520 RTM Resin System  (discontinued **)
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: CYCOM® PR 520 RTM is a one-part, 180°C (355°F) curing epoxy resin system offering superior damage tolerance and good strain to failure required for composite primary structure applications. The value of resin infusion is the ability to design complex geometric parts while leveraging a unitized structure which ultimately leads to a reduction in weight, lower part counts and the elimination of many post-manufacturing processes. CYCOM PR 520 RTM is an off-white thick paste at room temperature reducing to a low viscosity when heated for injection. The resin has a low enough viscosity to allow injection at 90 – 100°C (194 – 212°F). Following injection, the resin viscosity decreases with increasing tool temperature to below 50 cP, thus helping to ensure full fiber wetting. CYCOM PR 520 RTM resin is fully cured following a 2-hour dwell at 180°C (355°F) after which it has a continuous hot/wet service temperature of 104°C (220°F). For reinforcement preforming operations, a fully compatible binder system, CYCOM® 7720 RTM, and a low areal weight film, PR 520-1, have been developed for use with CYCOM PR 520 RTM. The binder and low areal weight film are available pre-coated onto fabrics of the customer’s choice. A separate datasheet for CYCOM 7720 RTM is available upon request.

Features & Benefits:

  • One-part epoxy resin system
  • 30 day out-life at room temperature
  • Two year shelf-life at -18°C (0°F)
  • Low exotherm, i.e., thick part production capable
  • ~500 cP initial injection viscosity
  • <30 cP minimum viscosity
  • Full cure after 2 hours at 180°C (355°F)
  • Continuous hot/wet service performance >104°C (220°F)
  • Low moisture absorption, ~0.6%
  • High resin toughness
  • Fully compatible binder available
Applications: Primary structure applications requiring superior toughness
  • Engine Blades
  • Engine Blade Spacers/Platforms
  • Containment Cases
  • Outer Guide Vanes
  • Hinge/Brackets/Fittings

Information provided by Cytec, subsequently acquired by Solvay.

Vendors:
Available Properties
  • Density, Cured Neat Resin
  • Tensile Strength, Neat Resin
  • Tensile Strength, Open Hole
  • Tensile Strength, Warp
  • Elongation at Break, Neat Resin
  • Tensile Modulus, Neat Resin
  • Tensile Modulus, Warp
  • Flexural Strength, Neat Resin
  • Flexural Modulus, Neat Resin
  • Compressive Strength, Neat Resin
  • Compressive Strength, After 11.8 J/mm Impact
  • Compressive Strength, After 8.3 J/mm Impact
  • Compressive Strength, After 7.0 J/mm Impact
  • Compressive Strength, After 4.5 J/mm Impact
  • Compressive Strength, Warp
  • Compressive Strength, Open Hole, wet
  • Compressive Strength, Open Hole, wet
  • Compressive Strength, Open Hole
  • Compressive Modulus, Neat Resin
  • Compressive Modulus, Warp
  • Bearing Yield Strength
  • Poissons Ratio, Neat Resin
  • Fracture Toughness, SENB KIC, Neat Resin
  • Shear Modulus, Neat Resin
  • Shear Modulus, In-plane, wet
  • Shear Modulus, In-plane
  • Shear Strength, Neat Resin
  • Shear Strength, In-plane
  • Shear Strength, In-plane, wet
  • CTE, linear, by TMA
  • Maximum Service Temperature, Air, continuous hot/wet
  • Glass Transition Temp, Tg, Neat Resin
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Solvay, former Rhodia Engineering Plastics

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.