MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
AK Steel 410 Cb Martensitic Stainless steel
Categories: Metal; Ferrous Metal; Martensitic; Stainless Steel; T 400 Series Stainless Steel

Material Notes: AK Steel 410 Cb is an improved version of standard Type 410. The addition of columbium offers 3 major advantages: 1) Greater ease in heat treating, 2) Higher strength and toughness, 3) Improved grain size control.

Information provided by AK Steel

Vendors:
Available Properties
  • Density
  • Hardness, Rockwell B, Hardened at 1850°F for 30 min, oil quenched and tempered for 4 hrs at 1400°F [9.5 mm plate, transverse]
  • Hardness, Rockwell C, Hardened at 1850°F for 30 min, oil quenched and tempered for 4 hrs at 500°F [9.5 mm plate, transverse]
  • Hardness, Rockwell C, Hardened at 1850°F for 30 min, oil quenched and tempered for 4 hrs at 1000°F [9.5 mm plate, transverse]
  • Tensile Strength, Ultimate, Hardened at 1850°F for 30 min, oil quenched and tempered for 4 hrs at 1400°F [9.5 mm plate, transverse]
  • Tensile Strength, Ultimate, Hardened at 1850°F for 30 min, oil quenched and tempered for 4 hrs at 1000°F [9.5 mm plate, transverse]
  • Tensile Strength, Ultimate, Hardened at 1850°F for 30 min, oil quenched and tempered for 4 hrs at 500°F [9.5 mm plate, transverse]
  • Tensile Strength, Yield, Hardened at 1850°F for 30 min, oil quenched and tempered for 4 hrs at 1000°F [plate, transverse]
  • Tensile Strength, Yield, Hardened at 1850°F for 30 min, oil quenched and tempered for 4 hrs at 1000°F [plate, transverse]
  • Tensile Strength, Yield, Hardened at 1850°F for 30 min, oil quenched and tempered for 4 hrs at 1000°F [plate, transverse]
  • Elongation at Break, in 2 inches, Hardened at 1850°F for 30 min, oil quenched and tempered for 4 hrs at 1000°F [9.5 mm plate, transverse]
  • Elongation at Break, in 2 inches, Hardened at 1850°F for 30 min, oil quenched and tempered for 4 hrs at 500°F [9.5 mm plate, transverse]
  • Elongation at Break, in 2 inches, Hardened at 1850°F for 30 min, oil quenched and tempered for 4 hrs at 1400°F [9.5 mm plate, transverse]
  • Modulus of Elasticity
  • Charpy Impact, V-Notch, Hardened at 1850°F for 30 min, oil quenched and tempered for 4 hrs at 1000°F [9.5 mm plate, transverse]
  • Charpy Impact, V-Notch, Hardened at 1850°F for 30 min, oil quenched and tempered for 4 hrs at 500°F [9.5 mm plate, transverse]
  • Charpy Impact, V-Notch, Hardened at 1850°F for 30 min, oil quenched and tempered for 4 hrs at 1400°F [9.5 mm plate, transverse]
  • Electrical Resistivity
  • CTE, linear
  • CTE, linear
  • Thermal Conductivity
  • Thermal Conductivity
  • Carbon, C
  • Chromium, Cr
  • Iron, Fe, As Remainder
  • Manganese, Mn
  • Molybdenum, Mo
  • Niobium, Nb (Columbium, Cb)
  • Phosphorus, P
  • Silicon, Si
  • Sulfur, S
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

New MatWeb Services
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.