MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Poly-u-Mac Air-Cell T-100 Polyester Foam Core
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: Air-Cell is a hybrid, closed cell cross-linked polyester foam core that is an economical alternative to other cores used in the production of sandwich composite structures. In addition to its excellent strength to weight ratio, it offers good dimensional stability at elevated temperatures. Aircell T grade is available in a wide range of densities in order that designers, engineers and fabricators can select the most appropriate density for the prevailing application. It is suitable for a wide range of marine, road/rail transportation, aerospace and industrial applications. Poly-U-Mac offers a comprehensive kitting service for the Air-Cell product line with the capability to work directly from customers' CAD files. Used 'straight out of the box', Poly-U-Mac Air-Cell kits speed the manufacturing process, save labor costs and virtually eliminate material waste.

Key Features:

  • High strength to weight ratio
  • Good dimensional stability
  • Can be processed at up to 200°F
  • High 'in service' temperature performance
  • Does not absorb water
  • Compatible with most resins (polyester, epoxy and vinylester systems)
Typical Applications
  • Leisure & Commercial Marine: hulls, decks, stringers & bulkheads
  • Wind Energy: blades, cabins & spinners
  • Road: cabs, sleeper floors & RV bodies
  • Rail: train fronts, floors, cabs, exterior & interior paneling
  • Aerospace: flooring, toilet modules & overhead lockers

Information provided by Poly-u-Mac

Vendors:
Available Properties
  • Density, ASTM D1622
  • Tensile Strength, ASTM D1623
  • Flexural Strength, ASTM D790
  • Compressive Strength, ASTM D1621
  • Compressive Modulus, ASTM D1621-B
  • Poissons Ratio
  • Shear Modulus, ASTM C273
  • Shear Strength, ASTM C273
  • CTE, linear
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Processing Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.