MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Henkel Loctite® 222MS Low Strength/Small Screw Threadlocker
Categories: Polymer; Adhesive; Thermoset

Material Notes:
Threadlockers
Invented by Loctite Corporation to lock and seal threaded fasteners, Loctite® Liquid Threadlockers have found wide acceptance in a range of applications--from delicate electronic components to heavy construction equipment.

Loctite® Pre-Applied Threadlockers are dry-to-the-touch films applied to threaded fasteners by fastener suppliers and process centers located throughout North America. Ideally suited for OEMs, they improve speed of assembly and ensure quality by eliminating on-line adhesive dispensing.

Loctite® Threadlockers are available in varying viscosities and strengths for virtually any application, including exposure to extreme environments.

Loctite® 222MS Low Strength/Small Screw Threadlocker
Ideal for fastener diameters of 0.25" (6mm) and smaller. Controlled lubricity for accurate clamp loads. Parts can be separated using hand tools.

Torque capability, M10 steel nuts and bolts: 62 in. lbs. (break), 27 in. lbs. (prevail). Recommended Primer: 7649(N) or 7471(T) Mil-Spec (S-46163A) Type II, Grade M Typical Use: Easy removal small screws

Vendors:
Available Properties
  • Density
  • Viscosity, Thixotropic
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Cure Time
  • Cure Time, Full Cure; Steel
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Loctite Division of Henkel

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.