MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
SSAB Duroxite® 200 Abrasive Materials Deposited On Steel Backing Plate
Categories: Metal; Ferrous Metal

Material Notes: Duroxite 200 consists of specially formulated abrasive materials deposited on mild steel backing plate that is suitable for extremely severe abrasive wear and high to moderate impact applications. The overlay material is composed of primary chromium-rich carbides and refined multiple-alloy complex carbides dispersed evenly in a ductile eutectic austenite matrix. Duroxite 200 is available in single and double layers.

Key Benefits

  • Multiple-alloy complex carbides are harder and finer than chromium carbides and interlock between the primary chromium carbides to provide better wear resistance
  • Longer service life and better wear resistance compared to traditional chromium carbide overlay plate
  • Double-layer overlay maintains full wear resistance up to 600° C (1100° F)
Typical Applications: Duroxite 200 is widely used many industries including mining, cement, and steel. Some specific applications include:
  • Mining: Chutes, liner plates, conveyors sides, underground mine skips
  • Cement: Cement furnace components, sinter plant parts, fan blades, mixer blades, gyratory mantles, coal and cement pulverizer rolls, raw material crushing components, molding panels
  • Power: Ore sintering, crushing, riddling, blast furnace hoppers, throats, and ovens

Data provided by SSAB.

Vendors:
Available Properties
  • Hardness, Rockwell C, Single pass
  • Hardness, Rockwell C, Double passes
  • Hardness, Vickers, Single pass
  • Hardness, Vickers, Double passes
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
SSAB Tunnplat AB

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.