MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Online Metals
Visit Online Metals for fast service
on small quantity orders.
Elkem (Bluestar Silicones) BLUESIL™ RTV 6321 QC A/B Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Description: BLUESIL® RTV 3621 QC A/B is a two component silicone elastomer that cures at room temperature by polyaddition reaction, at a 1:1 ratio. It is designed to be used for molding in a variety of applications that require a faster cure, particularly those requiring realistic skin feel.

Applications:

  • Molding life like parts
  • Animatronics; special effect skins
  • Props for the film industry
  • Theme park props and reproduction molds
Features:
  • Easy to use viscosity
  • Translucent – can be pigmented
  • Quick Cure
  • Excellent reproduction of details
  • Excellent mechanical properties
  • Low linear shrinkage
  • High resistance to inorganic chemicals and ultraviolet rays

Information provided by Bluestar Silicones

Vendors:
Available Properties
  • Specific Gravity, TP 013, A
  • Specific Gravity, TP 013, B
  • Viscosity, A
  • Viscosity, B
  • Storage Temperature
  • Hardness, Shore A, ASTM D2240
  • Tensile Strength, ASTM D412
  • Elongation at Break, ASTM D412
  • Tear Strength, ASTM D624, Die B
  • Pot Life, NM 128
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.