MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.
Master Bond MasterSil 151Med Medical Grade Silicone Potting Compound
Categories: Polymer; Thermoset; Silicone

Material Notes: Description: Master Bond MasterSil 151Med is a two component, low viscosity silicone compound for high performance potting and encapsulation. MasterSil 151Med is an addition cured system and does not require exposure to air for complete cross-linking. It has a convenient ten to one mix ratio by weight, and will not outgas while curing. It is 100% solids and contains no solvents. MasterSil 151Med has an exceptionally low viscosity enabling it to be highly desirable for potting and encapsulation. First and foremost, MasterSil 151Med, as is true with silicones in general, offers flexibility and high temperature resistance. It has good electrical insulation properties. The system’s flexibility allows it to withstand severe thermal cycling and resist vibration and shock. MasterSil 151Med resists gamma radiation, ETO and various chemical sterilants. These properties enable this system to be well suited for medical applications involving optical and electrical components. It can also be used for encapsulating electronic circuitry, LEDs, optical fibers and other optical components in a wide array of medical devices. MasterSil 151Med is transparent and has a service temperature range of -65°F to +400°F. It fully passes USP Class VI testing for biocompatibility.

Product Advantages:

  • Addition cured; no by-products released during cure; does not require air for curing
  • Low exotherm; very long pot life; low viscosity ideal for potting and encapsulation
  • Readily cures at ambient temperatures or faster cure at elevated temperatures
  • Can cure in thicknesses beyond 1 inch
  • Very low shrinkage upon cure
  • Excellent optical clarity and transmission properties
  • Meets USP Class VI specification
  • Good electrical insulation properties; highly resistant to water
Key Features
  • Meets USP Class VI specifications
  • High flexibility
  • Optically clear
  • Serviceable from -65°F to +400°F
  • Electrically insulative
  • Low viscosity

Information provided by MasterBond®

Vendors:
Available Properties
  • Viscosity, Part B
  • Viscosity, Part A
  • Hardness, Shore A
  • Tensile Strength at Break
  • Elongation at Break
  • Shear Strength, Bond, Al to Al
  • Volume Resistivity
  • Dielectric Constant
  • Dielectric Strength
  • CTE, linear
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Refractive Index
  • Transmission, Visible, transparent; thickness not quantified
  • Cure Time
  • Cure Time
  • Pot Life, 100 gram batch
  • Shelf Life, in original unopened containers
  • USP Class VI
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Master Bond Inc.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.