MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
CHT Group QM 107 QSI Quantum Silicones 7 Durometer Condensation Cure Moldmaking Material
Categories: Polymer; Thermoset; Silicone

Material Notes: QM 107 is a two component, room temperature condensation cure silicone material. The cured rubber is very soft, has excellent mechanical properties and good shelf-life stability. This material is used to make large, intricate pattern, skin molds or where extreme flexibility and elasticity are required. A variety of catalysts are offered with this material. Complies with FDA indirect food contact regulation CFR 177.2600 when used with QM Cat Clear FG. refer to QM Cat Clear FG data sheet for typical properties.

Key Features:

  • Low Viscosity
  • Low durometer
  • Fast demold time
  • High elongation
Main Applications:
  • Molds for small statues, large statues and monument restoration
  • Molds for polyester, polyurethane and epoxy resin castings
  • Ideal for pad-printing

Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

Vendors:
Available Properties
  • Specific Gravity, Uncatalyzed, QM CAT RED 3
  • Specific Gravity, Uncatalyzed, QM CAT PURPLE
  • Specific Gravity, Uncatalyzed, QM CAT BLUE
  • Specific Gravity, catalyzed with QM CAT PURPLE
  • Specific Gravity, catalyzed with QM CAT RED 3
  • Specific Gravity, catalyzed with QM CAT BLUE
  • Specific Gravity, Base
  • Viscosity, Uncatalyzed, QM CAT PURPLE
  • Viscosity, Uncatalyzed, QM CAT BLUE
  • Viscosity, Uncatalyzed, QM CAT RED 3
  • Viscosity, catalyzed with QM CAT RED 3
  • Viscosity, catalyzed with QM CAT BLUE
  • Viscosity, catalyzed with QM CAT PURPLE
  • Viscosity, Base
  • Linear Mold Shrinkage, Cured
  • Storage Temperature, For 6 months
  • Hardness, Shore A, Cured
  • Hardness, Shore A, catalyzed with QM CAT RED 3
  • Hardness, Shore A, catalyzed with QM CAT BLUE
  • Hardness, Shore A, catalyzed with QM CAT PURPLE
  • Tensile Strength at Break, Cured
  • Elongation at Break, Cured
  • Tear Strength, B, Cured
  • Cure Time, Demold time, catalyzed with QM CAT RED 3
  • Cure Time, Demold time, catalyzed with QM CAT PURPLE
  • Cure Time, Demold time, catalyzed with QM CAT BLUE
  • Tack-Free Time, Catalyzed with QM CAT RED 3
  • Tack-Free Time, Catalyzed with QM CAT PURPLE
  • Tack-Free Time, Catalyzed with QM cat BLUE
  • Pot Life, catalyzed with QM CAT RED 3
  • Pot Life, catalyzed with QM CAT PURPLE
  • Pot Life, catalyzed with QM CAT BLUE
  • FDA
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.