MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
EOS MS1 Maraging Steel Sintered on EOSINT M 270
Categories: Metal; 3D Printing/Additive Manufacturing Metal; Ferrous Metal; Maraging Steel

Material Notes: Steel powder processed by DMSL. This steel has very good mechanical properties, and is easily heat-treatable using a simple thermal age-hardening process to obtain excellent hardness and strength. This material is ideal for many tooling applications (DirectTool) such as tools for injection molding, die casting of light metal alloys, punching, extrusion etc., and also for high performance industrial and engineering parts, for example in aerospace and motor racing applications.

EOS®, EOSINT®, and DMLS® are registered trademarks of EOS GmbH. Information provided by Axis Prototyping.

Key Words: US classification 18% Ni Maraging 300, European 1.2709 and German X3NiCoMoTi 18-9-5
Vendors:
Available Properties
  • Density
  • Porosity, with standard processing parameters
  • Hardness, Rockwell C, as built
  • Hardness, Rockwell C, after age hardening
  • Tensile Strength, Ultimate, as built
  • Tensile Strength, Ultimate, after age hardening
  • Tensile Strength, Yield, as built
  • Tensile Strength, Yield, after age hardening
  • Elongation at Break, after age hardening
  • Elongation at Break, as built
  • Modulus of Elasticity
  • Charpy Impact, Notched; after age hardening
  • Charpy Impact, Notched; as built
  • Specific Heat Capacity, as built
  • Specific Heat Capacity, after age hardening
  • Thermal Conductivity, as built
  • Thermal Conductivity, after age hardening
  • Maximum Service Temperature, Air
  • Shrinkage, age hardening
  • Aluminum, Al
  • Carbon, C
  • Chromium, Cr
  • Cobalt, Co
  • Iron, Fe, as balance
  • Manganese, Mn
  • Molybdenum, Mo
  • Nickel, Ni
  • Phosphorus, P
  • Silicon, Si
  • Sulfur, S
  • Titanium, Ti
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Electro Optical Systems GMBH

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.